US 5,891,269 A#3495381 Most Cited · 23 citations0.8/yr · PR 2.89ExpiredUS · Utility
Method of compacting anodized metals with lithium and fluoride-containing solutions without using heavy metals
Inventors: Koerner Torsten, Kresse Josef, Lindener Juergen, Roland Wolf-achimAssignee: Henkel KgaaFiled 1996-06-29 · Granted 1999-04-06

A process for sealing anodized metals without using any heavy metals comprises a first step in which the anodized metal is contacted for a period of between 3 and 30 minutes (for an anodized layer thickness of 20 μm) with an aqueous solution which has a temperature from 15° to…

US 6,059,897 A#6256158 Most Cited · 15 citations0.6/yr · PR 2.93ExpiredUS · Utility
Short-term heat-sealing of anodized metal surfaces with surfactant-containing solutions
Inventors: Koerner Torsten, Kresse JosefAssignee: Henkel KgaaFiled 1997-05-22 · Granted 2000-05-09

Process for post-sealing anodized metal surfaces, characterized in that the anodized metal is contacted with an aqueous solution for a period of between 0.5 and 2 minutes per micrometer of anodized coating thickness, which solution is at a temperature of between 75° C. and its…

US 5,935,656 A#8176837 Most Cited · 12 citations0.4/yr · PR 2.87ExpiredUS · Utility
Short duration hot seal for anodized metal surfaces
Inventors: Koerner Torsten, Kresse Josef, Roland Wolf-achim, Lindener JuergenAssignee: Henkel KgaaFiled 1996-10-09 · Granted 1999-08-10

A process for sealing anodized metal surfaces is characterized by bringing the anodized metal into contact with an aqueous solution at a temperature from 75° C. to the boiling point of the solution for a time equal to from 0.5 to 2 minutes per micrometer of anodized layer…

DE 19,524,828 A1#26311994 Most Cited · 4 citations0.1/yr · PR 1.22PendingDE · Application
Verfahren zum schwermetallfreien Verdichten anodisierter Metalle mit Lithium- und Fluorid-haltigen Lösungen

The invention concerns a method of compacting anodized metals without using heavy metals. The method is characterized in that: a) in a first step, the anodized metal is brought into contact for a period of between 3 and 30 minutes (for an anodizing layer thickness of 20 mu m)…

DE 19,538,777 A1#26141645 Most Cited · 4 citations0.1/yr · PR 1.23PendingDE · Application
Anodic oxide coating sealing process

Compaction of anodised metal surfaces - comprises bringing the anodised metal into contact with an aqueous solution heated to between 90 deg C and its b.pt. and having a pH of 5.5 - 8.5, for a length of time equal to 1 - 2 minutes per micron of anodised layer thickness. The…

CA 2,226,418 A1#44179931 Most Cited · 2 citations0.1/yr · PR 0.91PendingCA · Application
Process for sealing anodized metals with lithium- and fluoride-containing solutions free from heavy metals

The invention concerns a method of compacting anodized metals without using heavy metals. The method is characterized in that: a) in a first step, the anodized metal is brought into contact for a period of between 3 and 30 minutes (for an anodizing layer thickness of 20 µm) with…

WO 9,714,828 A1#56606480 Most Cited · 1 citations0.0/yr · PR 0.80PendingWO · Application
Short duration hot seal for anodised metal surfaces

The process for sealing anodised metal surfaces is characterised in that the anodised metal is brought into contact with an aqueous solution for a duration equivalent to 0.5-2 minutes per micron of anodised layer thickness. The solution has a temperature of between 75 DEG C and…

WO 9,746,738 A1#59850244 Most Cited · 1 citations0.0/yr · PR 0.77PendingWO · Application
Short-term heat-sealing of anodized metal surfaces with surfactant-containing solutions
Inventors: Koerner Torsten, Kresse JosefAssignee: Henkel Kgaa, Koerner TorstenFiled 1997-05-22

Described is a method of sealing anodized metal surfaces, the method being characterized in that the anodized metal is brought in contact, for a length of time between 0.5 and 2 minutes per micrometre of anodized-layer thickness, with an aqueous solution having a temperature…

CA 2,235,476 A1#114837987 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Short duration heat sealing of anodized metal surfaces

The process for sealing anodised metal surfaces is characterised in that the anodised metal is brought into contact with an aqueous solution for a duration equivalent to 0.5-2 minutes per micron of anodised layer thickness. The solution has a temperature of between 75 ~C and its…

CA 2,257,253 A1#153840564 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Short time hot sealing of anodized metal surfaces with surfactant-containing solutions
Inventors: Koerner Torsten, Kresse JosefAssignee: Henkel KgaaFiled 1997-05-22

Process for post-sealing anodized metal surfaces, characterized in that the anodized metal is contacted with an aqueous solution for a period of between 0.5 and 2 minutes per micrometer of anodized coating thickness, which solution is at a temperature of between 75°C and its…

EP 0,837,956 A1#73980437 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Method of compacting anodized metals with lithium and fluoride-containing solutions without using heavy metals

The invention concerns a method of compacting anodized metals without using heavy metals. The method is characterized in that: a) in a first step, the anodized metal is brought into contact for a period of between 3 and 30 minutes (for an anodizing layer thickness of 20 νm) with…

EP 0,857,227 A1#127661291 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Short duration hot seal for anodised metal surfaces

The process for sealing anodised metal surfaces is characterised in that the anodised metal is brought into contact with an aqueous solution for a duration equivalent to 0.5-2 minutes per micron of anodised layer thickness. The solution has a temperature of between 75 °C and its…

EP 0,902,849 A1#67683824 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Short-term heat-sealing of anodized metal surfaces with surfactant-containing solutions
Inventors: Koerner Torsten, Kresse JosefAssignee: Henkel KgaaFiled 1997-05-22

Described is a method of sealing anodized metal surfaces, the method being characterized in that the anodized metal is brought in contact, for a length of time between 0.5 and 2 minutes per micrometre of anodized-layer thickness, with an aqueous solution having a temperature…

MX 9,800,083 A#138776294 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredMX · Utility
Method of compacting anodized metals with lithium and fluoride-containing solutions without using heavy metals.

The invention concerns a method of compacting anodized metals without using heavy metals. The method is characterized in that: a) in a first step, the anodized metal is brought into contact for a period of between 3 and 30 minutes (for an anodizing layer thickness of 20…

WO 9,703,232 A1#68776135 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method of compacting anodized metals with lithium and fluoride-containing solutions without using heavy metals

The invention concerns a method of compacting anodized metals without using heavy metals. The method is characterized in that: a) in a first step, the anodized metal is brought into contact for a period of between 3 and 30 minutes (for an anodizing layer thickness of 20 νm) with…