The process for sealing anodised metal surfaces is characterised in that the anodised metal is brought into contact with an aqueous solution for a duration equivalent to 0.5-2 minutes per micron of anodised layer thickness. The solution has a temperature of between 75 DEG C and…
Assignee / Organization
Koerner Torsten
2Total Forward Citations
3Indexed Patents
1Avg Citations / Patent
1Portfolio H-Index
Described is a method of sealing anodized metal surfaces, the method being characterized in that the anodized metal is brought in contact, for a length of time between 0.5 and 2 minutes per micrometre of anodized-layer thickness, with an aqueous solution having a temperature…
The invention concerns a method of compacting anodized metals without using heavy metals. The method is characterized in that: a) in a first step, the anodized metal is brought into contact for a period of between 3 and 30 minutes (for an anodizing layer thickness of 20 νm) with…