PCT No. PCT/EP94/01513 Sec. 371 Date Jan. 29, 1996 Sec. 102(e) Date Jan. 29, 1996 PCT Filed May 10, 1994 PCT Pub. No. WO94/26790 PCT Pub. Date Nov. 24, 1994Support for catalysts, containing at least two constituents chosen from silica, alumina and aluminium phosphate, having a…
Koch Benoit
Ethylene polymer having a die swell ratio (R B ) of at least 1.4, a resistance to crazing under stress (ESCR) of at least 55 h and a melt index (MI 5 ) of at least 0.2 g/10 min. Processes for obtaining this ethylene polymer using different catalytic systems, the first based on…
Catalyst support containing at least two components chosen among silica, alumina and aluminium phosphate, with a specific surface of 100 to 800 m<2>/g, a crystallization temperature higher or equal to 700 DEG C, a pore volume of 1.5 to 4 cm<3>/g, and the relationship…
PCT No. PCT/EP94/01514 Sec. 371 Date Feb. 2, 1996 Sec. 102(e) Date Feb. 2, 1996 PCT Filed May 10, 1994 PCT Pub. No. WO94/26791 PCT Pub. Date Nov. 24, 1994Process for the manufacture of a support containing silica and at least one constituent chosen from alumina and aluminium…
Ethylene polymers having a swelling index of at least 1.4, a resistance to cracking under load (ESCR) of at least 55 h and a melt index (M15) of at least 0.2 g/10 min.., Pref. the ethylene polymer may contain 0.1-10 wt.% of a comonomer chosen from butene, hexene and mixt. of…
The present invention relates to a process for the manufacture of a support containing silica and at least one constituent chosen from alumina and aluminium phosphate, according to which an alcohol, water, a silicon alkoxide and an acid are mixed under conditions such that…
Olefin polymerisation catalyst system comprising a solid catalyst component based on Cr on a support contg. silica, alumina and Al phosphate and an organoaluminium cpd. cocatalyst.
A polyethylene composition suitable for making into caps and closures is described, which has a density of 950 - 960 kg/m 3 , a SHI (1/100) of 4 - 12,, a melt index MI 2 between 0.2 and 2 g/10 min, and a relationship between spiral flow 'SF' (measured in mm at 250°C/1000…
Process for the production of a support containing silica and at least one component chosen among alumina and aluminium phosphate, consisting of mixing an alcohol, water, a silicon alcoholate and an acid in such conditions that the gelification or precipitation of silica is…
A process for the preparation of an activated catalyst for the polymerization of olefins, includes mixing, in the absence of a solvent, at least one chromium salt with a support composition including at least one compound (A) which is an inorganic, oxygen-containing compound of…
Copolymers of ethylene and α-olefins are provided having (a) a density (D) in the range 0.900 - 0.940 g/cm3, (b) a melt index MI 2 (2.16 kg, 190°C) in the range of 0.01 - 50 g/10 min, (c) a melt index MI 2 (2.16 kg, 190°C) and Dow Rheology Index (DRI) satisfying the equation…
A polyethylene composition suitable for making into caps and closures is described, which has a density of 950-960 kg/m 3 , a SHI (1/100) of 4-12, a melt index MI 2 between 0.2 and 2 g/10 min, and a relationship between spiral flow ‘SF’ (measured in mm at 250° C./1000 bar/100…
Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a first polymer is made in suspension in a first reactor and 80-20 wt % of a second polymer is made in suspension in a second reactor in the presence of the first…
A polyethylene composition having a good balance of strength, flexibility and processability is disclosed, comprising (a) 40-55 wt% of a copolymer fraction (A) comprising ethylene and a C 4 -C 10 alpha-olefin, and having an MI 2 of from greater than 300 to 800 g/10min or a Mw of…
The invention discloses a slurry process for ethylene polymerization, which comprises one in seriesIn a reactor system of one or more reactors, characterized by an average polymerization productivity [ kgPE/kg catalyst ] of r1 at any first residence time during operation]A1 is…
Process for the manufacture of a support for olefin polymerization catalysts comprising silica, aluminium phosphate and optionally alumina, according to which a source of silica, chosen from alkaline aqueous silica sols and alkaline aqueous solutions of inorganic silicate, is…
Process for the manufacture of a support containing silica and at least one constituent chosen from alumina and aluminum phosphate, according to which an alcohol, water, a silicon alkoxide and an acid are mixed under conditions such that gelling or precipitation of silica is…
Ethylene polymer having a blow-up ratio (R B ) of at least 1.4, a resistance to crazing under stress (ESCR) of at least 55 h and a melt index (MI 5 ) of at least 0.2 g/10 min. Processes for obtaining this ethylene polymer using different catalytic systems, the first based on…
The olefin polymerization catalyst comprises a supported transition metal, magnesium and halogen; the support comprises aluminum phosphate and at least one oxide of silica or alumina. The catalyst is formed by impregnating the support with a liquid complex formed by reacting a…
A polyethylene composition suitable for making into caps and closures is described, which has a density of 950 - 960 kg/m3, a SHI(1/100) of 4-12,a melt index MI2 between 0.2 and 2 g/10 min, and a relationship between spiral flow 'SF' (measured in mm at 250DEG/1000…
Process for the preparation of a catalyst support according to which an inorganic powder including silica is impregnated with a solution, in an alcohol, of an alcoholate of a transition metal chosen from groups IVB and VB of the Periodic Table, the hydrocarbon radical of the…
본 발명에서는, 950 - 960 kg/m 3 의 밀도, 4~12 의 SHI (1/100) , 0.2 내지 2 g/10 min 의 용융 지수 MI 2 , 및 E > 200 - SF 의 나선형 유동 'SF' (250 ℃/1000 bar/100mm/s 에서 mm 로 측정됨) 와 ESCR 'E' (시간으로 측정됨) 사이의 관계를 갖거나, 대안적으로는 950-960 kg/m 3 의 밀도, 4-12 의 SHI (1/100) , 0.2 내지 2 g/10 min 의 용융…
Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a first polymer is made in suspension in a first reactor and 80-20 wt % of a second polymer is made in suspension in a second reactor in the presence of the first…
Process for producing a multimodal polyethylene in at least two loop reactors connected in series, in which 20-80wt% of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80wt% of a low molecular weight (LMW) polymer is made in suspension in a…
A domestic PEF cooking appliance (11) having: a food container (12) which can be filled with a liquid (W), having opposing PEF electrodes (6 a, 4 b) between which a food product (G) can be introduced; a PEF signal generator (5) for applying a PEF Signal (PS) to the PEF…