Patents
WO 9,426,790 A1#2797775 Most Cited · 26 citations0.8/yr · PR 6.02PendingWO · Application
Catalyst support, method for making a precursor gel for a catalyst support

Catalyst support containing at least two components chosen among silica, alumina and aluminium phosphate, with a specific surface of 100 to 800 m<2>/g, a crystallization temperature higher or equal to 700 DEG C, a pore volume of 1.5 to 4 cm<3>/g, and the relationship…

WO 9,426,791 A1#9229229 Most Cited · 11 citations0.3/yr · PR 2.39PendingWO · Application
Process for the preparation of a catalyst support, catalyst for olefin polymerization and process for the polymerization of olefins with said catalyst

Process for the production of a support containing silica and at least one component chosen among alumina and aluminium phosphate, consisting of mixing an alcohol, water, a silicon alcoholate and an acid in such conditions that the gelification or precipitation of silica is…

WO 2011/089112 A1#10819036 Most Cited · 10 citations0.7/yr · PR 1.59PendingWO · Application
Novel polymers

Copolymers of ethylene and α-olefins are provided having (a) a density (D) in the range 0.900 - 0.940 g/cm3, (b) a melt index MI 2 (2.16 kg, 190°C) in the range of 0.01 - 50 g/10 min, (c) a melt index MI 2 (2.16 kg, 190°C) and Dow Rheology Index (DRI) satisfying the equation…

US 8,202,951 B2#15754639 Most Cited · 7 citations0.5/yr · PR 1.55ActiveUS · Utility
Slurry phase polymerisation process
Inventors: Koch Benoit, Marissal Daniel, Parisel Marc, Walworth Brent RAssignee: Koch Benoit, Marissal DanielFiled 2008-08-29 · Granted 2012-06-19

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a first polymer is made in suspension in a first reactor and 80-20 wt % of a second polymer is made in suspension in a second reactor in the presence of the first…

WO 2012/010690 A1#15809165 Most Cited · 7 citations0.5/yr · PR 1.53PendingWO · Application
Polyethylene composition

A polyethylene composition having a good balance of strength, flexibility and processability is disclosed, comprising (a) 40-55 wt% of a copolymer fraction (A) comprising ethylene and a C 4 -C 10 alpha-olefin, and having an MI 2 of from greater than 300 to 800 g/10min or a Mw of…

US 2010190921 A1#24719846 Most Cited · 4 citations0.2/yr · PR 1.39PendingUS · Application
Slurry phase polymerisation process

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a first polymer is made in suspension in a first reactor and 80-20 wt % of a second polymer is made in suspension in a second reactor in the presence of the first…

WO 2009/030647 A1#26982072 Most Cited · 4 citations0.2/yr · PR 1.13PendingWO · Application
Slurry phase polymerisation process

Process for producing a multimodal polyethylene in at least two loop reactors connected in series, in which 20-80wt% of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80wt% of a low molecular weight (LMW) polymer is made in suspension in a…

US 8,772,426 B2#32794722 Most Cited · 3 citations0.2/yr · PR 1.08ActiveUS · Utility
Polymers

Copolymers of ethylene and α-olefins having (a) a density (D) in the range 0.900-0.940 g/cm 3 , (b) a melt index MI 2 (2.16 kg, 190° C.) in the range of 0.01-50 g/10 min, (c) a melt index MI 2 (2.16 kg, 190° C.) and Dow Rheology Index (DRI) satisfying the equation [DRI/MI 2…

WO 2009/030646 A1#45322415 Most Cited · 2 citations0.1/yr · PR 0.87PendingWO · Application
Slurry phase polymerisation process

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80wt% of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80wt% of a low molecular weight (LMW) polymer is made in suspension in a…

WO 9,818,834 A1#45220107 Most Cited · 2 citations0.1/yr · PR 0.87PendingWO · Application
Copolymer of ethylene and of at least one alpha-olefin and method for obtaining same
Inventors: Koch BenoitAssignee: Solvay, Koch BenoitFiled 1997-10-16

The invention concerns a copolymer of ethylene and of at least one alpha-olefin obtained by means of a catalytic solid with chromium oxide base deposited on an inorganic support, said copolymer having an index of fluidity HLMI measured in g/10 min, an amount Q of alpha-olefin,…

US 2012289665 A1#61952150 Most Cited · 1 citations0.1/yr · PR 0.74PendingUS · Application
Novel polymers

Copolymers of ethylene and α-olefins are provided having (a) a density (D) in the range 0.900-0.940 g/cm3, (b) a melt index MI 2 (2.16 kg, 190° C.) in the range of 0.01-50 g/10 min, (c) a melt index MI 2 (2.16 kg, 190° C.) and Dow Rheology Index (DRI) satisfying the equation…

US 9,279,023 B2#61901083 Most Cited · 1 citations0.1/yr · PR 0.74ActiveUS · Utility
Slurry phase polymerisation process
Inventors: Marissal Daniel, Koch Benoit, Moineau ChristopheAssignee: Marissal Daniel, Koch BenoitFiled 2012-06-21 · Granted 2016-03-08

Process for polymerizing ethylene in a reactor system containing one or more reactors in series, having a characteristic such that the average polymerization productivity [kgPE/kgcata] per unit ethylene per hour a1 during operation at any first residence time r1 is less than 1.7…

US 2010249344 A1#137781784 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Slurry phase polymerisation process

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80 wt % of a low molecular weight (LMW) polymer is made in suspension in a…

US 2010273960 A1#76977489 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Slurry phase polymerisation process

Process for producing a multimodal polyethylene in at least two loop reactors connected in series, in which 20-80 wt % of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80 wt % of a low molecular weight (LMW) polymer is made in suspension…

US 2013109812 A1#132268193 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Polyethylene composition

A polyethylene composition having a good balance of strength, flexibility and processability is disclosed, comprising (a) 40-55 wt % of a copolymer fraction (A) comprising ethylene and a C 4 -C 10 alpha-olefin, and having an MI 2 of from greater than 300 to 800 g/10 min or a Mw…

US 2014142260 A1#87796717 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Slurry phase polymerisation process

A slurry process for the polymerisation of ethylene is disclosed, which takes place in a reactor system comprising one or more reactors in series, having a characteristic such that the average polymerisation productivity [kg PE/kgcata] per unit ethylene per hour aI during…

US 8,183,332 B2#117095687 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Slurry phase polymerisation process
Inventors: Koch Benoit, Marissal Daniel, Parisel Marc, Walworth Brent RAssignee: Koch Benoit, Marissal DanielFiled 2008-08-29 · Granted 2012-05-22

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80 wt % of a low molecular weight (LMW) polymer is made in suspension in a…

US 8,183,333 B2#91518341 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Slurry phase polymerisation process
Inventors: Koch Benoit, Marissal Daniel, Parisel Marc, Walworth Brent R, Frederich AndreAssignee: Koch Benoit, Marissal DanielFiled 2008-08-29 · Granted 2012-05-22

Polymerisation process in which polyethylene is produced in slurry in a polymerisation reactor in the presence of a Ziegler Natta catalyst and an activator, and a stream or slurry containing the polymer is withdrawn from the reactor and transferred to a flash tank operating at a…

US 8,183,334 B2#104931369 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Slurry phase polymerisation process
Inventors: Koch Benoit, Marissal Daniel, Parisel Marc, Walworth Brent RAssignee: Koch Benoit, Marissal DanielFiled 2008-08-29 · Granted 2012-05-22

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80 wt % of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80 wt % of a low molecular weight (LMW) polymer is made in suspension in a…

US 8,202,950 B2#106162539 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Slurry phase polymerisation process
Inventors: Koch Benoit, Marissal Daniel, Parisel Marc, Walworth Brent RAssignee: Koch Benoit, Marissal DanielFiled 2008-08-29 · Granted 2012-06-19

Process for producing a multimodal polyethylene in at least two loop reactors connected in series. In the process 20-80 wt % of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80 wt % of a low molecular weight (LMW) polymer is made in…

WO 2009/030642 A1#106440627 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Slurry phase polymerisation process

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80wt% of a high molecular weight (HMW) polymer is made in suspension in a first reactor and 20-80wt% of a low molecular weight (LMW) polymer is made in suspension in a…

WO 2009/030644 A1#138927714 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Slurry phase polymerisation process

A polymerisation process is disclosed in which polyethylene is produced in slurry in a polymerisation reactor in the presence of a Ziegler Natta catalyst and an activator, and slurry containing the polymer is withdrawn from the reactor and transferred to a flash tank operating…

WO 2009/030645 A1#65273130 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Slurry phase polymerisation process

Process for producing a multimodal polyethylene in at least two reactors connected in series, in which 20-80wt% of a first polymer is made in suspension in a first reactor and 80-20wt% of a second polymer is made in suspension in a second reactor in the presence of the first…

WO 2012/175632 A1#132610564 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Slurry phase polymerisation process

A slurry process for the polymerisation of ethylene is disclosed, which takes place in a reactor system comprising one or more reactors in series, having a characteristic such that the average polymerisation productivity [kgPE/kgcata] per unit ethylene per hour al during…