The present invention provides high temperature compositions comprising blends of a first polymer, poly(aryl ether ketone phthalazinone)s, and a second polymer, selected from poly(aryl ether ketone)s, poly(aryl ketone)s, poly(ether ether ketone)s, poly(ether ketone ketone)s, or…
Hsu Tim
The present invention is directed to an extrudable resin composition and a method of extruding the extrudable resin composition, comprising a high temperature engineering thermoplastic, one or more reinforcement components, an enhancing filler component, a polymeric lubricant,…
Compositions and methods for a melt processable semicrystalline poly(aryl ether ketone) incorporating phthalazinone and 4,4′-biphenol as comonomer units are described herein. The polymers are resistant to and insoluble in common organic solvents and liquids as well as in…
Compositions and methods for a melt processable semicrystalline poly(aryl ether ketone) incorporating phthalazinone and 4,4′-biphenol as comonomer units are described herein. The polymers are resistant to and insoluble in common organic solvents and liquids as well as in…
Substrate protective structures, including high performance polymers and polymer coatings from 1 to over 2500 mils thick, are disclosed. The structures protect metal and other surfaces with heat resistant, abrasion resistant, and chemical inert polymers. The structures are…
The present invention is directed to an extrudable resin composition and a method of extruding the extrudable resin composition, comprising a high temperature engineering thermoplastic, one or more reinforcement components, an enhancing filler component, a polymeric lubricant,…
Substrate protective structures, including high performance polymers and polymer coatings from 1 to over 2500 mils thick, are disclosed. The structures protect metal and other surfaces with heat resistant, abrasion resistant, and chemical inert polymers. The structures are…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
A sealed mat system that protects an environment from discharge of a fluid or a solid material is disclosed as well as a method for deploying the sealed mat system. The sealed mat system for spill containment comprises interconnected channels, seals, and a composite panel…
A watertight coupler, of which the watertight structure is firm and reliable to make the coupler able to fast and conveniently connect two mutually opposite water pipes. The watertight coupler comprises a main body with a specific axial length; the main body of the coupler has…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
The present invention is directed to an extrudable resin composition and a method of extruding the extrudable resin composition, comprising a high temperature engineering thermoplastic, one or more reinforcement components, an enhancing filler component, a polymeric lubricant,…
A sealed mat system that protects an environment from discharge of a fluid or a solid material is disclosed. The mat system comprises interconnected channels, seals, and a composite panel structure.
본 발명은 제1 고분자인 폴리(아릴 에테르 케톤 프탈아진온) 및 폴리(아릴 에테르 케톤), 폴리(에테르 에테르 케톤), 폴리(에테르 케톤 케톤), 또는 폴리벤즈이미다졸, 열가소성 폴리이미드, 폴리에테르이미드, 폴리(아릴 에테르 설폰), 폴리(페닐렌 설파이드) 및 이들의 조합으로 이루어진 그룹으로부터 선택된 제2 고분자의 블렌드들을 포함하는 고온 조성물들을 제공한다. 상기 조성물은 향상된 고온 특성, 예를 들면, 향상된 고온 하중 지지력 및 향상된 고온 용융 가공성을 갖는다.
The present invention provides high temperature compositions comprising blends of a first polymer, poly(aryl ether ketone phthalazinone)s, and a second polymer, selected from poly(aryl ether ketone)s, poly(aryl ketone)s, poly(ether ether ketone)s, poly(ether ketone ketone)s, or…
The present invention provides high temperature compositions comprising blends of a first polymer, poly(aryl ether ketone phthalazinone)s, and a second polymer, selected from poly(aryl ether ketone)s, poly(aryl ketone)s, poly(ether ether ketone)s, poly(ether ketone ketone)s, or…
The present invention provides high temperature compositions comprising blends of a first polymer, poly(aryl ether ketone phthalazinone)s, and a second polymer, selected from poly(aryl ether ketone)s, poly(aryl ketone)s, poly(ether ether ketone)s, poly(ether ketone ketone)s, or…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
The present invention provides high temperature compositions comprising blends of a first polymer, poly(aryl ether ketone phthalazinone)s, and a second polymer, selected from poly(aryl ether ketone)s, poly(aryl ketone)s, poly(ether ether ketone)s, poly(ether ketone ketone)s, or…
Anti-seepage tank with variable capacity Abstract The present techniques relate to an anti-seepage tank with a variable capacity, the tank comprising a tank body, wherein the tank body is composed of a plurality of combined plates, and two adjacent combined plates are connected…
Claimed is a process for producing a melt blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK) which comprises the steps of: pre-dry-mixing a PBI with a PEKK to obtain a dry mix; feeding said dry mix to an extruder with a plurality of heating zones; setting said…
PROBLEM TO BE SOLVED: To provide a method for producing a solution blend of a polybensimidazole (PBI) and a polyetherketoneketone (PEKK).SOLUTION: The PBI is mixed with sulfuric acid at a temperature between 40-80°C for 30 minutes to 2 hours to produce a PBI solution, and the…
Polyolefins having the same or different functional groups covalently bound to the polyolefin, such as polyolefins having hindered phenol groups bound thereto, can be prepared by from a maleic anhydride modified polyolefin, with or without a coupling agent, and a hindered phenol…
Melt stable polyaryletherketoneketone are prepared by from a reactive, lower molecular weight polyaryletherketoneketone having an ultraviolet absorbance at 455 nm of at least 0.185 when measured in 0.1% solution in dichloroaeetic acid.