A hollow fiber membrane has an outer layer of polybenzimidazole (PBI) and an inner support layer, e.g., polyetherimide (PEI). The hollow fiber membrane is made by a co-extrusion (spinning) process. The hollow fiber membrane may be used in a pervaporation process, such as a…
Gruender Michael
A pervaporation membrane may be an acid-resistant polybenzidimazole (PBI) membrane. The acid-resistant PBI membrane may be a PBI membrane chemically modified by a process selected from the group consisting of sulfonation, phosphonation, cross-linking, N-substitution, and/or…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
A porous polybenzimidazole (PBI) particulate resin is disclosed. This resin is easily dissolved at ambient temperatures and pressures. The resin is made by: dissolving a virgin PBI resin in a highly polar solvent; precipitating the dissolved PBI in a bath; and drying the…
PBI compositions include solutions comprising PBI and acrylate monomer and coatings comprising PBI and polyacrylate. The solutions may also include polymerization initiator, solvent, co-polymers. The coatings are thermally resistant, electrically insulating (dielectric), and…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
A coating is a mixture of polybenzimidazole polymer and an epoxy. The coating may further include a primer underlying the coating. The coating may further include an adhesion promoter. A solution includes a polybenzimidazole polymer, an epoxy resin, an initiator, and a carrier…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
A polymer blend comprises PBI, PAEK, and PEI. A method of making the foregoing blend comprises the steps of intimately blending PBI, PAEK, and PEI by dissolving PBI, PAEK, and PEI in a strong acid or melt blending PBI, PAEK, and PEI.
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
The polymer mixture comprises polybenzimidazole (PBI)/polyvinylbutyral (PVB). The weight ratio (PVB:PBI) of this mixture may range from 0.25-50:50-99.75 or 15-85:15-85. The coating is based upon the polymer mixture.
A coating is a mixture of polybenzimidazole polymer and an epoxy. The coating may further include a primer underlying the coating. The coating may further include an adhesion promoter. A solution includes a polybenzimidazole polymer, an epoxy resin, an initiator, and a carrier…
A process for producing a solution blend of a polybenzimidazole (PBI) and a polyetherketoneketone (PEKK). The PBI is mixed with sulfuric acid at a temperature between 40° C. and 80° C. for 30 minutes to 2 hours to produce a PBI solution then cooled to room temperature to form a…
PBI compositions include solutions comprising PBI and acrylate monomer and coatings comprising PBI and polyacrylate. The solutions may also include polymerization initiator, solvent, co-polymers. The coatings are thermally resistant, electrically insulating (dielectric), and…
A pervaporation membrane may be an acid-resistant polybenzidimazole (PBI) membrane. The acid-resistant PBI membrane may be a PBI membrane chemically modified by a process selected from the group consisting of sulfonation, phosphonation, cross-linking, N-substitution, and/or…
The polymer mixture comprises polybenzimidazole (PBI)/polyvinylbutyral (PVB). The weight ratio (PVB:PBI) of this mixture may range from 0.25-50:50-99.75 or 15-85:15-85. The coating is based upon the polymer mixture.