Ethanol is prepared by hydrogenating acetic acid under superatmospheric pressure and at elevated temperatures by a process wherein a predominantly cobalt-containing catalyst is used and acetic acid and hydrogen are passed through the reactor, at from 210° to 330° C. and under…
Hoeppner Bernd
Herstellung von Ethanol durch Hydrierung von Essigsäure unter erhöhtem Druck und bei erhöhter Temperatur, indem man hierzu einen überwiegend Cobalt enthaltenden Katalysator als Kontakt verwendet und daß man Essigsäure und Wasserstoff im Bereich von 210 bis 330°C und 10 bis 350…
Acicular cobalt-containing magnetic iron oxides having a high coercive force and a core/shell structure and hence a low temperature-dependence of the coercive force are prepared by a process in which, in a first stage, surface activation is effected by means of iron(II) and…
Acicular cobalt-containing magnetic iron oxides having a high coercive force and a core/shell structure and hence low temperature dependence of the coercive force are prepared by a process in which, in a first stage, surface activation is effected by means of iron(II) and cobalt…
Finely divided, needle-like magnetic CrO2 modified with Fe, Te and/or Sb has a coercive field strength of at least 40 kA/m, a saturation magnetisation of at least 85 nTm<3>/g, and a specific surface area (SSA) of a least 25 m<2>/g. A temp. dependent drop of remanent…
Acicular cobalt-containing magnetic iron oxide composed of a core of an iron oxide of the formula FeO1.33-1.5 and a cobalt-enriched surface layer is improved with regard to the stability of the magnetic properties by a coating of silicon compound and aluminium compound applied…
A finely divided acicular CrO 2 modified with iron, tellurium and/or antimony and having a high coercive force possesses improved heat stability of the residual induction and a relatively narrow distribution of the particle size and of the coercive force. This CrO 2 pigment is…
The invention relates to a process for producing acicular cobalt-containing magnetic iron oxide, which is improved with regard to the stability of the magnetic properties by a coating of silicon and aluminium compounds applied to the particle surface. This coating is carried out…
The invention relates to a process for preparing high-coercitivity acicular (needle-shaped) cobalt-containing magnetic iron oxides having a core-shell structure and low temperature dependence of the coercive force resulting therefrom, wherein, in a first step, a surface…