Preparation of acicular cobalt-containing magnetic iron oxide
Abstract
Acicular cobalt-containing magnetic iron oxides having a high coercive force and a core/shell structure and hence low temperature dependence of the coercive force are prepared by a process in which, in a first stage, surface activation is effected by means of iron(II) and cobalt ions under alkaline conditions on the iron oxide core under an inert gas atmosphere and thereafter, in a second stage, an epitactic coating of cobalt ferrite is applied, which coating is formed oxidatively from iron (II) and cobalt (II) hydroxide, likewise under alkaline reaction conditions. The total amount of cobalt ions used for doping remains unchanged compared with the known doped iron oxides or is even smaller. In the second process stage, the achievable coercive force can be controlled by the proportion of air in the gas mixture during the formation of the epitactic coating.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 3.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A process for the preparation of acicular magnetic iron oxide having a core/shell structure, consisting of a core of iron oxide and a ferrite shell containing cobalt (II) and iron(II) ions, which process comprises: in a first stage, depositing an iron(II) and cobalt hydroxide precipitate under an inert gas atmosphere on a suspension of acicular magnetic iron oxide by precipitation of iron(II) and cobalt(II) ions under alkaline conditions, and then in a second stage, depositing an iron(II) and cobalt hydroxide precipitate on the gamma-iron oxide treated in the first stage, by adding a further s
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗