A method for welding a gamma-prime precipitation strengthened alloy component. In one aspect the welding process includes preheating the alloy component to minimize the difference in contraction between the weld deposit and the substrate portion of the component during…
Fuesting Timothy P
A process for producing a fine grain forged superalloy article having a high yield strength at intermediate temperatures. A preferred starting composition comprises, by weight, 15% Cr, 13.6% Co, 4.1% Mo, 4.6% Ti, 2.2% Al, 0.01% C, 0.007% B, 0.07% Zr, balance Ni. This material is…
Superalloy castings having large variations in section thickness are heat treated using a cyclic stress relief procedure, with the temperature being cycled between about 50° F. (28° C.) and 150° F. (83° C.) below the second phase particle solvus temperature, to relieve the…
A process for producing a fine grain forged superalloy article having a high yield strength at intermediate temperatures. A preferred starting composition comprises, by weight, 15 % Cr, 13.6 % Co, 4.1 % Mo, 4.6 % Ti, 2.2 % Al, 0.01 % C, 0.007 % B, 0.07 % Zr, balance Ni. This…
A process for producing a fine grain forged superalloy article having a high yield strength at intermediate temperatures. A preferred starting composition comprises, by weight, 15 % Cr, 13.6 % Co, 4.1 % Mo, 4.6 % Ti, 2.2 % Al, 0.01 % C, 0.007 % B, 0.07 % Zr, balance Ni. This…
본 발명은 중간 온도에서 고항복 강도를 갖는 단조된 미세한 입자의 초합금 제품을 생산하는 방법에 관한 것이다. 양호한 초기 성분조성은 중량으로 15%Cr, 13.6%Co, 4.1%Mo, 4.6%Ti, 2.2%Al, 0.01%C, 0.007%B, 0.07%Zr, 그나머지 Ni를 포함한다. 이 재료는 γ프라임 솔버스 이상의 온도와 약 0.5의 진변형에서 단조된다. 또한, 이 재료는 중간 슈퍼솔버스 소둔과 함께 γ프라임 솔버스 온도 이하로 단조 될 수 있다. 그후, 과시효된 재료는 γ프라임 솔버스…
On décrit un procédé pour produire un article en superalliage forgé à grain fin présentant une résistance à la déformation élevée à des températures intermédiaires. Une composition de départ préférée comprend, en poids, 15 % Cr, 13,6 % Co, 4,1 % Mo, 4,6 % Ti, 2,2 % Al, 0,01 % C,…
A process for producing a fine grain forged superalloy article having a high yield strength at intermediate temperatures. A preferred starting composition comprises, by weight, 15 % Cr, 13.6 % Co, 4.1 % Mo, 4.6 % Ti, 2.2 % Al, 0.01 % C, 0.007 % B, 0.07 % Zr, balance Ni. This…
A multi-piece radial turbine rotor includes a hub, turbine blades, and a flowpath ring that couples the turbine blades to the hub. Joints between the components of the rotor are adapted for inspection during manufacture to identify potential defects in the joints.
A multi-piece radial turbine rotor includes a hub, turbine blades, and an intermediate ring that couples the turbine blades to the hub. Joints between the components of the rotor are adapted for inspection during manufacture to identify potential defects in the joints.
A radial turbine rotor incorporating ceramic matrix composite turbine blades is disclosed. The radial turbine rotor can include a dovetail shape retention features for coupling the ceramic matrix composite turbine blades to a central hub.
A radial turbine rotor incorporating ceramic matrix composite turbine blades is disclosed. The radial turbine rotor can include a dovetail shape retention features for coupling the ceramic matrix composite turbine blades to a central hub.