Superalloy forging process
Abstract
A process for producing a fine grain forged superalloy article having a high yield strength at intermediate temperatures. A preferred starting composition comprises, by weight, 15% Cr, 13.6% Co, 4.1% Mo, 4.6% Ti, 2.2% Al, 0.01% C, 0.007% B, 0.07% Zr, balance Ni. This material is forged at a temperature above the gamma prime solvus and at a true strain of at least 0.5. Alternately, the material may be forged below the gamma prime solvus temperature with intermediate super solvus anneals. The overaged material is then worked at a temperature below the gamma prime solvus. The resultant fine grain material is then heat treated or can be further isothermally forged prior to heat treatment to produce complex shapes.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 15 · Forward citations: 25.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
Process for producing an article having a fine grain size and good mechanical properties at temperatures below about 1200° F., starting with a material consisting essentially of (by wt. %) 12-20% Cr, 10-20% Co, 2-5.5% Mo, 3-7% Ti, 1.2-3.5% Al, 0.005-0.25% C, 0.005-0.05% B, 0.01-0.1% Zr, 0-1% Ta, 0-4.5% W, 0-1% Nb, 0-2.0% Fe, 0-0.3% Hf, 0-0.02% Y, 0-0.1% V, 0-1.0% Re, balance Ni, and having a gamma prime solvus temperature, consisting of the steps of: a. working the material in at least one step selected from the group consisting of (i) working above the gamma prime solvus, (ii) working below t
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗