A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
Epler Mario
A precipitation hardenable cobalt-nickel based superalloy is disclosed. The formula is characterized by comprising the following components in percentage by weight: the balance of the alloy is cobalt and common impurities. The alloy provides a novel combination of strength and…
A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
A nickel base superalloy powder for additive manufacturing applications is disclosed. The alloy powder has the following broad weight percent composition: C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 4-16 Fe 0-1.5 Mo 0-6 W 0-8 Co 0-15 Ti 0-2 A1 0.5-5.5 Nb 0-6 Ta 7.5-14.5 Hf 0-2.0 Zr 0-0.1…
A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
A nickel base superalloy powder for additive manufacturing applications is disclosed. The alloy powder has the following broad weight percent composition: C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 4-16 Fe 0-1.5 Mo 0-6 W 0-8 Co 0-15 Ti 0-2 A1 0.5-5.5 Nb 0-6 Ta 7.5-14.5 Hf 0-2.0 Zr 0-0.1…
A method for fabricating an article includes forming a billet consisting essentially of a stainless steel composition of manganese 2.00 wt.% – 24.00 wt.% chromium 19.00 wt.% – 30 wt.% molybdenum 0.50 wt.% – 4.0 wt.% nitrogen 0.25 wt.% – 1.10 wt.% carbon ≤0.08 wt.% phosphorus…
Se describe una superaleación a base de cobalto y níquel endurecible por precipitación. Se caracteriza por la siguiente composición porcentual en peso. C aproximadamente 0,01 a aproximadamente 0,15 Cr aproximadamente 6,00 a aproximadamente 15,00 Ni aproximadamente 30,00 a…
석출 경화성의 코발트-니켈 베이스 초합금이 개시된다. 이 합급은 하기의 중량 퍼센트 조성을 특징으로 한다: 합금의 나머지는 코발트 및 일반적인 불순물이다. 상기 합금은 가스 터빈 및 제트 엔진에서 발견되는 높은 작동 온도에 장기간 노출된 후에도 강도와 연성의 새로운 조합을 제공한다. 이 합금으로부터 제조된 세립 강철 물품이 또한 개시된다. 상기 강철 물품은 또한 높은 작동 온도에서 산화로부터 합금을 보호하는 Al 2 O 3 및 Cr 2 O 3 의 연속적인 표면층을 특징으로 한다.
부가적 제조 적용들을 위한 니켈-계 초내열합금 분말이, 개시된다. 합금 분말은, 뒤따르는 넓은 중량 퍼센트 조성을 갖는다: C 0-0.1, Mn 0.5 최대, Si 0-0.03, Cr 4-16, Fe 0-1.5, Mo 0-6, W 0-8, Co 0-15, Ti 0-2, Al 0.5-5.5, Nb 0-6, Ta 7.5-14.5, Hf 0-2.0, Zr 0-0.1, Re 0-6, Ru 0-3, B 0-0.03. 합금의 나머지는, 적어도 니켈 및 일반적인 불순물들이다. 합금으로 이루어지는 제조…
물품 제조 방법은, 기본적으로 망간 2.00 wt.% 내지 24.00 wt.%, 크롬 19.00 wt.% 내지 30 wt.%, 몰리브덴 0.50 wt.% 내지 4.0 wt.%, 질소 0.25 wt.% 내지 1.10 wt.%, 탄소 ≤ 1 wt.%, 인 ≤ 0.03 wt.%, 황 ≤ 1 wt.%, 니켈 < 22 wt.%, 코발트 < 0.10 wt.%, 실리콘 ≤ 1 wt.%, 니오븀 ≤ 0.80 wt.%, 산소 ≤ 1 wt.%, 구리 ≤ 0.25 wt.%, 잔부가 철인 스테인리스강…
A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
A method for fabricating an article includes forming a billet consisting essentially of a stainless steel composition of manganese 2.00 wt. %-24.00 wt. % chromium 19.00 wt. %-30 wt. % molybdenum 0.50 wt. %-4.0 wt. % nitrogen 0.25 wt. %-1.10 wt. % carbon ≤1 wt. % phosphorus ≤0.03…
A nickel base superalloy powder for additive manufacturing applications is disclosed. The alloy powder has the following broad weight percent composition: C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 4-16 Fe 0-1.5 Mo 0-6 W 0-8 Co 0-15 Ti 0-2 Al 0.5-5.5 Nb 0-6 Ta 7.5-14.5 Hf 0-2.0 Zr 0-0.1…
A nickel base superalloy powder for additive manufacturing applications is disclosed. The alloy powder has the following broad weight percent composition: C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 4-16 Fe 0-1.5 Mo 0-6 W 0-8 Co 0-15 Ti 0-2 Al 0.5-5.5 Nb 0-6 Ta 7.5-14.5 Hf 0-2.0 Zr 0-0.1…
A nickel base superalloy powder for additive manufacturing applications is disclosed. The alloy powder has the following broad weight percent composition: C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 4-16 Fe 0-1.5 Mo 0-6 W 0-8 Co 0-15 Ti 0-2 Al 0.5-5.5 Nb 0-6 Ta 7.5-14.5 Hf 0-2.0 Zr 0-0.1…
A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
A method for fabricating an article includes forming a billet consisting essentially of a stainless steel composition ofmanganese 2.00 wt. %-24.00 wt. %chromium 19.00 wt. %-30 wt. %molybdenum 0.50 wt. %-4.0 wt. %nitrogen 0.25 wt. %-1.10 wt. %carbon ≤1 wt. %phosphorus ≤0.03 wt.…
A low coefficient of thermal expansion high strength alloy and methods of formation thereof, the alloy including: chromium 7 wt. % to 10 wt. %; molybdenum 20 wt. % to 25 wt. %; tungsten 4 wt. % to 7 wt. %; aluminum 0.5 wt. % to 2 wt. %; titanium 0.5 wt. % to 2 wt. %; boron 0.005…
A precipitation hardenable, cobalt-nickel base superalloy is disclosed. The is characterized by the following weight percent composition. C about 0.01 to about 0.15 Cr about 6.00 to about 15.00 Ni about 30.00 to about 45.00 W about 3.00 to about 15.00 Ti about 0.50 to about 4.00…
A method for fabricating an article includes forming a billet consisting essentially of a stainless steel composition of manganese 2.00 wt.% – 24.00 wt.% chromium 19.00 wt.% – 30 wt.% molybdenum 0.50 wt.% – 4.0 wt.% nitrogen 0.25 wt.% – 1.10 wt.% carbon ≤0.08 wt.% phosphorus…
A low coefficient of thermal expansion high strength alloy and methods of formation thereof, the alloy including: chromium 7 wt.% to 10 wt.%; molybdenum 20 wt.% to 25 wt.%; tungsten 4 wt.% to 7 wt.%; aluminum 0.5 wt.% to 2 wt.%; titanium 0.5 wt.% to 2 wt.%; boron 0.005 wt.% to…