Ni-based superalloy powder for additive manufacturing and an article made therefrom
Abstract
A nickel base superalloy powder for additive manufacturing applications is disclosed. The alloy powder has the following broad weight percent composition: C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 4-16 Fe 0-1.5 Mo 0-6 W 0-8 Co 0-15 Ti 0-2 Al 0.5-5.5 Nb 0-6 Ta 7.5-14.5 Hf 0-2.0 Zr 0-0.1 Re 0-6 Ru 0-3 B 0-0.03 The balance of the alloy is at least 50% nickel and the usual impurities. An article of manufacture made from the alloy is also disclosed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 41 · Forward citations: 2.
Claims (10 — 2 Independent, 8 Dependent)
- Claim 1Independent Claim
A high γ ′ volume fraction Ni-base alloy for laser and electron beam additive manufacturing processes, said alloy consisting essentially of, in weight percent, C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 8-11 Fe 1 max. Mo 2-5 W 0.5-6 Co 4-6 Al 3-5 Nb 3.86-5 Ta 7.5-9.5 Hf 0-1.5 Zr 0-0.1 Ru 0-1 B 0-0.03 and the balance of the alloy is nickel and impurities found in commercial grades of Ni-base superalloys intended for the same use and service, said impurities including not more than 0.03% P, and not more than 0.01% each of S, O, and N; wherein % W+% Mo+% Ru+% Re ≤ 10; 10.5 ≤ % Nb+% Ta ≤ 14.5; wherein the alloy excludes titanium and rhenium; and wherein the alloy contains at least 50% nickel.
- Claim 2Depends on #1
The alloy claimed in claim 1 which contains at least about 9% Cr.
- Claim 3Depends on #1
The alloy claimed in claim 1 which contains at least about 3.5% W.
- Claim 4Depends on #3
The alloy claimed in claim 3 which contains not more than about 4.5% W.
- Claim 5Depends on #1
The alloy claimed in claim 1 which contains not more than about 4% Nb.
- Claim 6Depends on #1
An article of manufacture made from consolidated alloy powder produced from the alloy claimed in claim 1, wherein said article consists essentially of a γ phase matrix containing a γ ′ strengthening phase and the γ ′ phase is present in a volume fraction greater than 35%.
- Claim 7Depends on #6
The article claimed in claim 6 wherein the volume fraction of the γ ′ phase is greater than 50%.
- Claim 8Depends on #6
The article claimed in claim 6 which is further characterized by having a lattice misfit parameter (δ) that is greater than about − 0.1%, wherein the lattice misfit parameter is defined as: δ = 2 × (α γ ′ - α γ) α γ ′ + α γ and wherein α γ ′ is the lattice constant for the γ ′ precipitate and α γ is the lattice constant for the γ phase matrix material.
- Claim 9Independent Claim
A high γ ′ volume fraction Ni-base alloy for laser and electron beam additive manufacturing processes, said alloy consisting essentially of, in weight percent, C 0-0.1 Mn 0.5 max. Si 0-0.03 Cr 4-11 Fe 1 max. Mo 0-5 W 0.5-8 Co 0-6 Al 3-3.95 Nb 3.86-5 Ta 7.5-9.5 Hf 0-1.5 Zr 0-0.1 Re 0-1 Ru 0-1 B 0-0.03 and the balance of the alloy is nickel and impurities found in commercial grades of Ni-base superalloys intended for the same use and service, said impurities including not more than 0.03% P, and not more than 0.01% each of S, O, and N; wherein % W+% Mo+% Ru+% Re ≤ 10; 10.5 ≤ % Nb+% Ta ≤ 14.5; wherein the alloy excludes titanium; and wherein the alloy contains at least 50% nickel.
- Claim 10Depends on #9
The alloy claimed in claim 9 wherein rhenium is excluded.
Technical Overview & Description
CROSS REFERENCE TO RELATED APPLICATIONS This application is a continuation of U.S. patent application Ser. No. 16/750,745, filed Jan. 23, 2020, which claims the benefit of U.S. Provisional Patent Application No. 62/795,618, filed Jan. 23, 2019, the entireties of which are incorporated herein by reference. BACKGROUND OF THE INVENTION Field of the Invention This invention relates generally to Ni-based superalloys and in particular to a Ni-based superalloy powder that is useful in an additive manufacturing process for making articles therefrom. Description of the Related Art With the advent of additive manufacturing technologies, manufacturers of turbomachinery (high temperature gas turbines and jet engines are looking at leveraging the design flexibility offered by the additive manufacturing process to directly produce parts with complex features for use in the hot gas path of gas turbines and jet engines. A powder bed fusion technique using selective laser melting is one of the most promising additive manufacturing techniques. Compared with the known electron beam powder bed process, selective laser melting with powder bed does not require pre-sintering. Consequently, designers can incorporate complex internal features in the parts without worrying about removing sintered powder trapped inside hollows of the part after printing. Laser systems also offer finer resolution for printing intricate features. The drawback of laser melting system is the large temperature gradient that occurs in a part during solidification. The very large temperature gradient leads to cracking of the alloy, especially for superalloys having a high volume fraction of the gamma prime ( γ ′ ) phase that provides superior strength and creep resistance such as CM247LC and Rene142. For selective laser melting process, cracking occurs either during build or post-build heat treatment. Efforts have been made by the superalloy research community to mitigate the cracking problem, but have focused prima
Cited By — Indexed Forward Citations (2 of 2 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 12,742,227 B2 | Nickel-based alloy | 2026 | 0 |
| US 12,799,565 B2 | Nickel-based alloy | 2026 | 0 |
References Cited — Backward Prior Art (41)
Non-Patent Literature (10)
- B.A. Cowles et al.,
- “
- Cyclic Behavior of Turbine Disk Alloys at 650C,
- ”
- ASME Trans., vol. 102, Oct. 1980, pp. 356-363.
- R. Vilar et al.,
- “
- Repair and manufacturing of single crystal Ni-based superalloys components by laser powder deposition
- —
- A review,