A solder ball having a diameter of 1.2 mm or less, a dispersion of a diameter distribution of 5% or less and sphericity of 0.95 or more, an area ratio of the maximum dendrite being 80% or less of a cross section including a center of the solder ball, comprises a first additional…
Date Masayoshi
PROBLEM TO BE SOLVED: To provide a lead-free solder ball which is capable of correctly controlling the growth behavior of the intermetallic compound formed at the boundaries with the terminal surfaces of metallized packages and printed circuit boards by a solder alloy and Ni and…
A solder ball having a diameter of 1.2 mm or less, a dispersion of a diameter distribution of 5% or less and sphericity of 0.95 or more, an area ratio of the maximum dendrite being 80% or less of a cross section including a center of the solder ball, comprises a first additional…
<P>PROBLEM TO BE SOLVED: To provide solder balls composed mostly of Sn with Ag and Cu added, which solve such problems caused by discoloration at the time of soldering such as the poor loading ratio of the solder balls, and defects in determining damaged solder bumps,…
<P>PROBLEM TO BE SOLVED: To provide a manufacturing method of solder ball which enables an efficient and stable addition of minor additional elements to increase reliability of solder bonding interface. <P>SOLUTION: A study result on a method for minute addition of…
<P>PROBLEM TO BE SOLVED: To improve joining strength by inhibiting decrease in the thickness of terminals in electronic component parts equipped with terminals whose main component is Ag. <P>SOLUTION: A solder alloy is used which contains 3.0-5.0% Ag and 1.0% or less…
A manufacturing method for a cold-working die, in which steel ingots of a cold-work tool steel are hot worked and made into a base material. The cold-work tool steel comprises, by mass, 0.6-1.2% of C; 0.8-2.5% of Si; 0.4-2.0% of Mn; 0.03-0.1% of S; 5.0-9.0% of Cr; 0.5-2.0% of Mo…
<P>PROBLEM TO BE SOLVED: To provide a solder and solder ball for connection of lead-free electronic device and the electronic device using it, which can suppress growth of an intermetallic compound formed in the boundary between a package metallized with a soldering…
<P>PROBLEM TO BE SOLVED: To increase the joining strength in a soldered electronic component, and to improve the operational reliability of electronic equipment in various using environments. <P>SOLUTION: A trace amount of one or more selected from Fe, Ni and Co as…
Disclosed is a Pb-free solder alloy consisting of, in mass%, 0.1-1.5% of Ag, 0.5-0.75% of Cu, Ni in an amount satisfying 12.5 ≤ Cu/Ni ≤ 100, and the balance of Sn and unavoidable impurities. The solder alloy preferably contains, in mass%, 0.3-1.2% of Ag and 0.01-0.04% of Ni.…
<P>PROBLEM TO BE SOLVED: To provide an Sb based solder alloy essentially consisting of Sn and solving both the problem of defects caused by the yellowing and the reduction of metallic luster upon the formation of a solder ball or the formation of a solder bump and the…
Provided are a Ni-based superalloy for stably obtaining high tensile strength and a method for manufacturing the same. A Ni-based superalloy having a composition of, in mass%, C: 0.10% or less, Si: 0.5% or less, Mn: 0.5% or less, P: 0.05% or less, S: 0.050% or less, Fe: 45% or…
<P>PROBLEM TO BE SOLVED: To solve problems such as a bad surface texture of a Sn-Cu alloy which leads to judgement of failure in visual examination and failure in mounting of solder balls, to provide a lead-free solder alloy, which is excellent in drop impact strength and…
PROBLEM TO BE SOLVED: To provide a metal core material both good in handling and low thermal expansion and further good in electrical conduction and thermal conduction, and to provide a metal core using it and a metal core substrate formed by using the metal core. SOLUTION: The…
<P>PROBLEM TO BE SOLVED: To provide a Pb-free brazing filler metal sheet which solves the problem of degradation in bonding reliability caused by voids in a brazing filler metal and a compound phase formed between particles. <P>SOLUTION: The brazing filler metal…
A manufacturing method for a cold-working die in which steel ingots of a cold-work tool steel are hot worked and made into a base material, the base material is quenched and tempered to a hardness of 58-62 HRC, and then machined into a die shape. The cold-work tool steel…
Provided are: a steel material which has a hardness of 58HRC or more and which is suitable for production of a cold working die; and processes for producing a steel material, a prehardened steel product and a cold working die respectively. The present invention pertains to a…
PROBLEM TO BE SOLVED: To provide a method for producing a ceramic sintered body, which can solve a problem that swelling, cracking or deformation occurs in a ceramic molded body or a degreased body in a degreasing step or firing step, and by which dimentional variation relative…
PROBLEM TO BE SOLVED: To provide a method for manufacturing a metal plate for a metal core printed wiring board and a method for manufacturing the metal core printed wiring board which make simple and inexpensive a process of manufacturing the metal core printed wiring board and…
PROBLEM TO BE SOLVED: To provide a metal sheet for a metal core base material and its manufacturing method by which the problem of a phenomenon of dimensional variation occurring at the application of piercing treatment to a cold rolled metal sheet and a phenomenon of…
<P>PROBLEM TO BE SOLVED: To provide a Pb-free solder alloy with which the strength of a joint boundary can be improved without damaging the fundamental mechanical properties and wettability of the conventional solder alloy, and to provide a solder ball. <P>SOLUTION:…
PROBLEM TO BE SOLVED: To provide a steel for a cold die providing high hardness of 58 HRC or more, further 60 HRC or more and excellent in machinability and to provide its manufacturing method.SOLUTION: A steel for a high hardness cold die contains, by mass%, C:0.6 to 1.2%,…
PURPOSE:To safely recover gaseous ammonia from a treatment chamber at low cost and to readily control the pressure in the treatment chamber. CONSTITUTION:A gaseous ammonia recovery passage 2 is led out from a treatment chamber 1 kept to a negative pressure and a blower 3 and a…
Provided are: a high-hardness pre-hardened cold-rolled tool steel for surface PVD, wherein problems of softening and deformation due to thermal processing during when subjected to surface PVD are improved; a method for producing the high-hardness pre-hardened cold-rolled tool…
<P>PROBLEM TO BE SOLVED: To provide a solder junction having joined strength for suppressing breakage of a Cu<SB>6</SB>Sn<SB>5</SB>phase formed in soldering electronic components or the like. <P>SOLUTION: In the solder junction formed on a Cu…