Patents
Assignee / Organization

Date Masayoshi

34Total Forward Citations
4Indexed Patents
8Avg Citations / Patent
3Portfolio H-Index
WO 2007/081006 A1#6225047 Most Cited · 15 citations0.8/yr · PR 3.07PendingWO · Application
Solder alloy, solder ball and solder joint using same

Disclosed is a Pb-free solder alloy consisting of, in mass%, 0.1-1.5% of Ag, 0.5-0.75% of Cu, Ni in an amount satisfying 12.5 ≤ Cu/Ni ≤ 100, and the balance of Sn and unavoidable impurities. The solder alloy preferably contains, in mass%, 0.3-1.2% of Ag and 0.01-0.04% of Ni.…

WO 2012/115025 A1#11637634 Most Cited · 9 citations0.6/yr · PR 2.09PendingWO · Application
Manufacturing method for cold-working die

A manufacturing method for a cold-working die in which steel ingots of a cold-work tool steel are hot worked and made into a base material, the base material is quenched and tempered to a hardness of 58-62 HRC, and then machined into a die shape. The cold-work tool steel…

WO 2012/043228 A1#15190018 Most Cited · 7 citations0.5/yr · PR 1.79PendingWO · Application
High-hardness pre-hardened cold-rolled tool steel for surface pvd, method for producing same, and surface pvd method for same
Inventors: Date Masayoshi, Nakatsu HideshiAssignee: Hitachi Metals Ltd, Date MasayoshiFiled 2011-09-14

Provided are: a high-hardness pre-hardened cold-rolled tool steel for surface PVD, wherein problems of softening and deformation due to thermal processing during when subjected to surface PVD are improved; a method for producing the high-hardness pre-hardened cold-rolled tool…

WO 2012/115024 A1#31213799 Most Cited · 3 citations0.2/yr · PR 1.17PendingWO · Application
Cold-work tool steel exhibiting superior machinability

A cold-work tool steel comprising, in mass%: 0.6 - 1.2% of C; 0.7 - 2.5% of Si; 0.3 - 2.0% of Mn; 0.02 - 0.1% of S; 3.0 - less than 5.0% of Cr; 0.5 - 2.0% of Mo and W independently or as a complex (Mo+1/2W); 0.04 - less than 0.3% of Al; and Fe and unavoidable impurities as the…