A method is provided for forming an anti-corrosive, oxide layer on steel. The steel surface is subjected to superheated steam for a period of one to several hours. Before subjecting the steel to the superheated steam, a clean steel surface is initially heated to at least 200° C.…
Inventor / Author Profile
Coester Erwin
28Total Forward Citations
8Indexed Patents
2Patent H-Index
Frequent Co-Inventors: Coester Erwin Dipl-phys Dr Coester, Erwin, Dipl.-phys. Dr., 5170 Juelich Coester Erwin Dr Krapf Heinz Krapf Heinz Dipl Ing Krapf, Heinz, Dipl.- Ing., 5171 Seglersdorf Mohrhauer Hans Pfistermeister Martin Pfistermeister Martin Dipl Che Pfistermeister, Martin, Dipl.-chem. Dr., 5160 Dueren Pfistermeister Martin Dr Sartor Bruno
A method is provided for forming an anti-corrosive oxide layer on steel. The steel surface is subjected to superheated steam for a period of one to several hours. Before subjecting the steel to the superheated steam, the steel surface is initially subjected to a gaseous formic…