Method for forming an anticorrosive oxide layer on steels
Abstract
A method is provided for forming an anti-corrosive oxide layer on steel. The steel surface is subjected to superheated steam for a period of one to several hours. Before subjecting the steel to the superheated steam, the steel surface is initially subjected to a gaseous formic acid atmosphere at a raised temperature of up to 480° C. The treatment with superheated steam takes place during a further heating period in which a temperature between 450° C. and 520° C. is maintained under steam flow-through conditions in which the steam flow has a Reynolds number greater than 900.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 10.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
In a method for forming an anti-corrosive oxide layer on steel, in which the steel surface is subjected to superheated steam for a period of at least one hour, the improvement comprising heating the steel surface to a temperature of above 180° C. up to 480° C. in a gaseous formic acid atmosphere, and then subjecting the heated steel to a further heating period of 1 to 5 hours in which a temperature between 450° C. and 520° C. is maintained, with superheated steam under flow conditions in which the flow has a Reynolds number of greater than 900.
- Claim 2Depends on #1
The method as defined in claim 1 wherein the formic acid is mixed with an inert gas as a carrier gas.
- Claim 3Depends on #2
The method as defined in claim 2 wherein the carrier gas is nitrogen or argon.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (10 of 10 total)
References Cited — Backward Prior Art (7)
Non-Patent Literature (1)
- Grobner et al., Chem. Zentralbl, (1960).