A method of manufacturing an article by consolidating powder material comprises forming a non-deformable tool ( 12 ) and a deformable tool ( 14 ). The non-deformable tool ( 12 ) comprises a plurality of tool parts ( 16,18 ). The non-deformable tool ( 12 ) defines a first cavity…
Voice Wayne E.
A method of correcting the shape of a brittle cast component such as a low pressure turbine blade. The method includes steps of placing the component against a creep mold having a surface defining the desired profile of the component and HIP treating it to creep deform the…
In order to avoid excessive internal stress and micro structure problems inherent with previous fusion welding techniques utilised for component structure fabrication, the present method creates a relatively thin in situ brazing alloy layer upon first and second component edges…
A first workpiece comprises a compressor disc ( 2 ) manufactured from a titanium alloy forging. A number of second workpieces, aerofoil blades ( 4 ), also forged from titanium alloy are arranged for attachment to the disc ( 2 ). The aerofoil blades ( 4 ) are evenly distributed…
A method of manufacturing a fan blade ( 26 ) for a gas turbine engine by powder metallurgy comprises the steps of forming a container ( 52 ) and placing at least one metal insert ( 52 ) at a predetermined position within the container ( 52 ) and filling the container ( 52 ) with…
A pocket ( 6 ) is machined into the surface of a component ( 9 ) by pressurising a fluid ( 1 ) and directing a jet ( 11 ) of the pressurized fluid ( 1 ) at the surface to be machined. Continuous relative movement is provided between the component ( 9 ) and the pressurized jet (…
The invention relates to a mould assembly for a hot isostatic pressing, HIP, process, comprising: an insert comprising a plurality of pieces which combine to provide a recess in which a protrusion of the component can be formed; and, a holding piece having at least one cavity in…
A method of forming a component ( 30 ) by isostatic pressing, the method comprising: providing a canister ( 4 ) suitable for isostatic pressing, the canister comprising first and second membranes ( 14, 16 ) which, in use, are disposed within the canister ( 4 ); the first and…
A component can be formed by a hot isostatic pressing (HIP) process but it is necessary to reinforce intricate internal structures against collapse and deformation by the hot isostatic pressing process. The present method utilises a low melting point salt or alloy reinforcement…
A method of manufacturing a blisk comprising a disc joined to an aerofoil, wherein a union piece of partially sintered powder and having an alignment feature is provided. The union piece is connected between the disc and the aerofoil, which is aligned relative to the disc by the…
A method of forming a fully consolidated joint between first and second components comprising the steps of forming a slot in the first component; inserting at least part of the second component into the slot; inserting a powder material into the slot; heating the powder material…
This invention relates to a mould assembly for a hot isostatic pressing, HIP, process for fabricating a component, comprising: a first part which includes a shaped surface for forming a first surface of the component, the shaped surface having at least one recess; a second part…
A method of manufacturing a metal component from metal powder comprises preparing ( 12 ) a metal powder, providing ( 14 ) gallium on at least part of the surface of at least some of the metal powder particles, encapsulating ( 16 ) the metal powder in a container, evacuating ( 18…
This invention relates to a mould assembly for a hot isostatic pressing, HIP, process for fabricating a component, comprising: a first part which includes a shaped surface for forming a first surface of the component, the shaped surface having at least one recess; a second part…
A gamma titanium aluminide alloy consisting of 46 at % aluminium, 8 at % tantalum and the balance titanium plus incidental impurities has an alpha transus temperature T α between 1310° C. and 1320° C. The gamma titanium aluminide alloy was heated to a temperature T 1 =1330° C.…
A component is manufactured from a powdered material such as a titanium alloy, by performing a first hot isostatic pressing HIP operation on the powdered material 14 while the powdered material is in contact with a molding surface 8 of a rigid, usable molding tool 2 . The first…
The present method creates a relatively thin in situ brazing alloy layer upon first and second component edges which are brought together in order to create a component joint. This in situ brazing alloy layer is created by deposition of brazing elements, such as copper or…