Abstract
A method of correcting the shape of a brittle cast component such as a low pressure turbine blade. The method includes steps of placing the component against a creep mold having a surface defining the desired profile of the component and HIP treating it to creep deform the component to the desired shape whilst consolidating it and removing gas and shrinkage porosity.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 35 · Forward citations: 11.
Claims (3 — 1 Independent, 2 Dependent)
- Claim 1Independent Claim
A method of forming a component comprising the steps of: a) casting a component comprising titanium aluminide alloy, forms of silicide based on niobium or molybdenum, or ceramic; b) placing the component adjacent a mould surface comprising yttria face coated alumina or silica; and c) creep deforming the component during the simultaneous application of heat and isostatic pressure to simultaneously consolidate the component and conform at least a part thereof to the mould surface.
- Claim 2Depends on #1
A method as claimed in claim 1 wherein the simultaneous application of hot isostatic pressure is applied via a secondary particulate material.
- Claim 3Depends on #2
A method as claimed in claim 2 wherein the component and mould surface are wrapped in a foil to prevent infiltration between the component and mould surface by the secondary particulate material.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (35)
Non-Patent Literature (2)
- Lapin, "Creep behaviour of a cast TiAl-based alloy for industrial applications," Intermetallics, vol. 14, 2006, pp. 115-122.
- Nicolai et al., "Investment Casting of Titanium," Titanium and Titanium Alloys: Fundamentals and Applications, 2003, pp. 263-271.