US 2011226390 A1#491716 Most Cited · 70 citations4.7/yr · PR 8.80PendingUS · Application
Superalloy Repair Welding Using Multiple Alloy Powders
Inventors: Chen Zheng, Timotin OvidiuAssignee: Chen Zheng, Timotin OvidiuFiled 2010-03-22

A method of welding a gas turbine engine substrate composed of a gamma prime precipitation strengthened nickel based superalloy, including the steps of: applying weld beads on the substrate to form a continuous layer the thickness of the weld beads; using a filler material made…

US 2010116793 A1#1921713 Most Cited · 33 citations2.1/yr · PR 6.33PendingUS · Application
Welded Repair of Defects Lying on the Inside of Components

The repair of cracks according to the state of the art comprises the fact that defects located on the inside must be worked outward in order to be able to be welded closed. The method according to the invention proposes not to work out cracks located on the inside, but to melt…

US 2012223057 A1#8138774 Most Cited · 12 citations0.9/yr · PR 3.01PendingUS · Application
Gas tungsten arc welding using flux coated electrodes

A method of applying a weld using a gas tungsten arc welding procedure. A filler element is provided to a welding location. The filler element includes a first material used during formation of a weld, and a second material that is capable of producing a slag upon melting…

US 8,561,298 B2#8537517 Most Cited · 12 citations0.9/yr · PR 2.07ActiveUS · Utility
Superalloy component welding at ambient temperature
Inventors: Morin James A, Iordache Lucian, Timotin Ovidiu, Oh SooyeumAssignee: Morin James A, Iordache LucianFiled 2008-02-29 · Granted 2013-10-22

A method for welding superalloy components at ambient temperature conditions while reducing the propensity of the superalloy material to crack as a result of the weld. A root pass region of the weld is formed using a filler material that exhibits ductility that is higher than…

WO 2008/098614 A1#9254401 Most Cited · 11 citations0.6/yr · PR 2.34PendingWO · Application
Welded repair of defects located on the inside

The repair of cracks according to the state of the art comprises the fact that defects located on the inside must be worked outward in order to be able to be welded closed. The method according to the invention proposes not to work out cracks located on the inside, but to melt…

US 2015050157 A1#12515665 Most Cited · 8 citations0.7/yr · PR 3.09PendingUS · Application
Hold and cool process for superalloy joining

Ni base superalloys containing relatively large amounts of Al and/or Ti are known to be difficult to weld satisfactorily. As the Al and Ti content of the superalloy is increased to improve the strength, the weldability of the component is drastically reduced. It is concluded…

US 8,324,526 B2#17153895 Most Cited · 6 citations0.4/yr · PR 1.84ActiveUS · Utility
Welded repair of defects lying on the inside of components
Inventors: Grueger Birgit, Iordache Lucian, Timotin OvidiuAssignee: Grueger Birgit, Iordache LucianFiled 2007-02-13 · Granted 2012-12-04

The repair of cracks according to the state of the art comprises the fact that defects located on the inside must be worked outward in order to be able to be welded closed. The method according to the invention proposes not to work out cracks located on the inside, but to melt…

US 8,618,434 B2#24467642 Most Cited · 4 citations0.3/yr · PR 1.42ActiveUS · Utility
Superalloy repair welding using multiple alloy powders
Inventors: Chen Zheng, Timotin OvidiuAssignee: Chen Zheng, Timotin OvidiuFiled 2010-03-22 · Granted 2013-12-31

A method of welding a gas turbine engine substrate composed of a gamma prime precipitation strengthened nickel based superalloy, including the steps of: applying weld beads on the substrate to form a continuous layer the thickness of the weld beads; using a filler material made…

WO 2013/070578 A1#32438384 Most Cited · 3 citations0.2/yr · PR 1.10PendingWO · Application
Hold and cool process for superalloy joining

Ni base superalloys containing relatively large amounts of Al and/or Ti are known to be difficult to weld satisfactorily. As the Al and Ti content of the superalloy is increased to improve the strength, the weldability of the component is drastically reduced. It is concluded…

WO 2012/119032 A1#50095562 Most Cited · 1 citations0.1/yr · PR 0.86PendingWO · Application
Gas tungsten arc welding using flux coated electrodes

A method of applying a weld using a gas tungsten arc welding procedure. A filler element is provided to a welding location. The filler element (14) includes a first material used during formation of a weld, and a second material that is capable of producing a slag upon melting…

US 9,347,124 B2#113468244 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Hold and cool process for superalloy joining
Inventors: Ozbaysal Kazim, Abdo Zafir A M, Timotin Ovidiu, Kamel AhmedAssignee: Ozbaysal Kazim, Abdo Zafir A MFiled 2012-06-06 · Granted 2016-05-24

Ni base superalloys containing relatively large amounts of Al and/or Ti are known to be difficult to weld satisfactorily. As the Al and Ti content of the superalloy is increased to improve the strength, the weldability of the component is drastically reduced. It is concluded…