Hold and cool process for superalloy joining
Abstract
Ni base superalloys containing relatively large amounts of Al and/or Ti are known to be difficult to weld satisfactorily. As the Al and Ti content of the superalloy is increased to improve the strength, the weldability of the component is drastically reduced. It is concluded herein that reducing the γ′ phase improves weldability. A stepwise, controlled heating and cooling process is described to be used in cooperation with a welding process to reduce the γ′ present and thereby improve weldability.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 12 · Forward citations: 0.
Claims (2 — 2 Independent, 0 Dependent)
- Claim 1Independent Claim
A nickel base superalloy, alloy 247, including a welded seam therein wherein said welded seam was produced by the process of: a) prior to welding, heating the weld location to an initial predetermined temperature above about 2100 deg. F. with a first heat source, b) welding said nickel base superalloy with a second heat source; and, c) removing said second heat source immediately upon completion of said welding; and, d) performing a controlled step cooling of said weld location such that no more than about 30 weight percent of the γ′ phase is formed at any hold temperature during the step cool
- Claim 2Independent Claim
A superalloy component assembly having therein the welded seam formed by the process of clai
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.