The invention includes a copper-comprising sputtering target. The target is monolithic or bonded and contains at least 99.99% copper by weight and has an average grain size of from 1 micron to 50 microns. The copper-comprising target has a yield strength of greater than or equal…
Strothers Susan
The invention includes components comprising an alloy containing a base metal and less than or equal to 30% alloying elements. The material has a grain size of less than or equal to about 30 microns and an absence of voids and inclusions of a size greater than 1 micron. The…
The invention includes a copper-comprising sputtering target. The target is monolithic or bonded and contains at least 99.99% copper by weight and has an average grain size of from 1 micron to 50 microns. The copper-comprising target has a yield strength of greater than or equal…
The invention includes methods of forming hollow cathode magnetron sputtering targets. A metallic material is processed to produce an average grain size of less than or equal to about 30 microns and subsequently subjected to deep drawing. The invention includes three-dimensional…
A sputtering target is described herein that comprises: a) a target surface component comprising a target material; b) a core backing component having a coupling surface and a back surface, wherein the coupling surface is coupled to the target surface component; and c) at least…
The invention includes a target construction having a sputtering region and a flange region laterally outward relative to the sputtering region. The flange region has a front surface disposed on a front face of the construction and a back surface opposing the front surface. An…
A sputtering target is described herein, which includes: a) a surface material, and b) a core material coupled to the surface material, wherein at least one of the surface material or the core material has less than 100 ppm defect volume. Methods for producing sputtering targets…
The invention encompasses a method of forming a metallic article. An ingot of metallic material is provided, and such ingot has an initial thickness. The ingot is subjected to hot forging. The product of the hot forging is quenched to fix an average grain size of less than 250…
Described is a method for producing a diffusion bonded sputtering target assembly which is thermally treated to precipitation harden the backing plate without compromising the diffusion bond integrity. The method includes heat treating and quenching to alloy solution and…
The invention includes physical vapor deposition targets formed of copper material and having an average grain size of less than 50 microns and an absence of course-grain areas throughout the target. The invention encompasses a physical vapor deposition target of a copper…
Sputtering targets having reduced burn-in times are described herein that include: a) a machine-finished surface material having an average grain size, and b) a core material having an average grain size, wherein the machine-finished surface material has an average surface…
Described is a method for producing a diffusion bonded sputtering target assembly which is thermally treated to precipitation harden the backing plate without compromising the diffusion bond integrity. The method includes heat treating and quenching to alloy solution and…
A sputtering target is described herein that comprises: a) a target surface component comprising a target material; b) a core backing component having a coupling surface and a back surface, wherein the coupling surface is coupled to the target surface component; and c) at least…
The invention includes methods by which hot isostatic pressing is utilized to form physical vapor deposition targets. In particular aspects, the physical vapor deposition targets can contain one or more of iridium, cobalt, ruthenium, tungsten, molybdenum, titanium, aluminum and…
A sputtering target is described herein that comprises: a) a target surface component comprising a target material; b) a core backing component having a coupling surface and a back surface, wherein the coupling surface is coupled to the target surface component; and c) at least…
The invention includes a copper-comprising sputtering target. The target is monolithic or bonded and contains at least 99.99% copper by weight and has an average grain size of from 1 micron to 50 microns. The copper-comprising target has a yield strength of greater than or equal…
The invention includes methods by which hot isostatic pressing is utilized to form physical vapor deposition targets. In particular aspects, the physical vapor deposition targets can contain one or more of iridium, cobalt, ruthenium, tungsten, molybdenum, titanium, aluminum and…
Methods for producing PVD sputtering targets comprising extended sidewalls are described that include: a) bonding a surface material to a core material to produce a rough part; b) forming the rough part; and in some embodiments, c) utilizing at least one machining step to form…
The invention encompasses a method of forming a metallic article. An ingot of metallic material is provided, and such ingot has an initial thickness. The ingot is subjected to hot forging. The product of the hot forging is quenched to fix an average grain size of less than 250…
The Invention includes target/backing plate constructions and methods of forming target/backing plate constructions. The targets and backing plates can be bonded to one another through an appropriate interlayer. The targets can comprise one or more of aluminum, copper, tantalum…
The invention includes a method of detecting impurities in a metal-containing article. A portion of metal material is removed from a metal article and is solubilized in an acid or base-comprising liquid to produce a liquid sample. The liquid sample is subjected to an incident…
The invention includes a physical vapor deposition target containing copper and at least two additional elements selected from Ag, Al, As, Au, B, Be, Ca, Cd, Co, Cr, Fe, Ga, Ge, Hf, Hg, In, Ir, Li, Mg, Mn, Nb, Ni, Pb, Pd, Pt, Sb, Sc, Si, Sn, Ta, Te, Ti, V, W, Zn and Zr, a total…
A sensor system has been developed for measuring erosion of a sputtering target (510) in a vacuum chamber that includes: a) a sputtering target, b) a wafer, c) a vacuum atmosphere located between the sputtering target and the wafer, and d) a sensor device (525) directly coupled…
Sputtering targets having reduced burn-in times are described herein that include: a) a machine-finished surface material having an average grain size, and b) a core material having an average grain size, wherein the machine-finished surface material has an average surface…
A sputtering target is described herein that comprises: a) a target surface component comprising a target material; b) a core backing component having a coupling surface and a back surface, wherein the coupling surface is coupled to the target surface component; and c) at least…