The invention includes backing plates having grain sizes of less than 10 microns and yield strengths of at least 30 ksi. The invention includes methods of producing backing plates by hot-forging, severe plastic deformation utilizing equal channel angular extrusion, and…
Ferrasse Stephane
Sputtering targets are described that comprise: a) a target surface component comprising a target material; b) a core backing component having a coupling surface, a back surface and at least one open area, wherein the coupling surface is coupled to at least part of the target…
The invention includes components comprising an alloy containing a base metal and less than or equal to 30% alloying elements. The material has a grain size of less than or equal to about 30 microns and an absence of voids and inclusions of a size greater than 1 micron. The…
The invention includes a copper-comprising sputtering target. The target is monolithic or bonded and contains at least 99.99% copper by weight and has an average grain size of from 1 micron to 50 microns. The copper-comprising target has a yield strength of greater than or equal…
A method of manufacturing an electrode, in which a solid metal material is extruded through a channel angular extrusion die to form the electrode. The solid metal material comprises copper and at least about 10 wt % zinc, and more particularly, between about 20 and about 40 wt %…
The invention includes methods of forming hollow cathode magnetron sputtering targets. A metallic material is processed to produce an average grain size of less than or equal to about 30 microns and subsequently subjected to deep drawing. The invention includes three-dimensional…
The invention includes a target construction having a sputtering region and a flange region laterally outward relative to the sputtering region. The flange region has a front surface disposed on a front face of the construction and a back surface opposing the front surface. An…
The invention includes backing plates having coolant deflectors with at least a portion of each of the deflectors being nonlinear. Projections projecting from the backing plate are configured to insert into openings within a sputtering target. The invention includes targets…
A material may include grains of sizes such that at least 99 % of a measured area contains grains that exhibit grain areas less than 10 times an area of a mean grain size of the measured area. As examples, at least 99 % of the measured area may contain grains with grain areas…
The invention includes backing plates having coolant deflectors with at least a portion of each of the deflectors being nonlinear. Projections projecting from the backing plate are configured to insert into openings within a sputtering target. The invention includes targets…
Sputtering targets are described that comprise: a) a target surface component comprising a target material; b) a core backing component having a coupling surface, a back surface and at least one open area, wherein the coupling surface is coupled to at least part of the target…
The invention includes a copper-comprising sputtering target. The target is monolithic or bonded and contains at least 99.99% copper by weight and has an average grain size of from 1 micron to 50 microns. The copper-comprising target has a yield strength of greater than or equal…
Sputtering targets are described that comprise: a) a target surface component comprising a target material; b) a core backing component having a coupling surface, a back surface and at least one open area, wherein the coupling surface is coupled to at least part of the target…
The invention includes a target construction having a sputtering region and a flange region (22). The flange region (22) has a protective layer (50) present over at least a portion of a front surface. The invention includes a sputtering target construction having a flange region…
The invention includes backing plates having grain sizes of less than 10 microns and yield strengths of at least 30 ksi. The invention includes methods of producing backing plates by hot-forging, severe plastic deformation utilizing equal channel angular extrusion, and…
The invention includes methods of forming hollow cathode magnetron sputtering targets. A metallic material is processed to produce an average grain size of less than or equal to about 30 microns and subsequently subjected to deep drawing. The invention includes three-dimensional…
A material may include grains of sizes such that at least 99 % of a measured area contains grains that exhibit grain areas less than 10 times an area of a mean grain size of the measured area. As examples, at least 99 % of the measured area may contain grains with grain areas…
The invention includes a target construction having a sputtering region and a flange region (22). The flange region (22) has a protective layer (50) present over at least a portion of a front surface. The invention includes a sputtering target construction having a flange region…
The invention includes backing plates having coolant deflectors with at least a portion of each of the deflectors being nonlinear. Projections projecting from the backing plate are configured to insert into openings within a sputtering target. The invention includes targets…
The invention includes methods of forming hollow cathode magnetron sputtering targets. A metallic material is processed to produce an average grain size of less than or equal to about 30 microns and subsequently subjected to deep drawing. The invention includes three-dimensional…