Patents
Assignee / Organization

Shaw Thomas M

141Total Forward Citations
56Indexed Patents
3Avg Citations / Patent
7Portfolio H-Index
US 8,076,756 B2#5457081 Most Cited · 17 citations1.1/yr · PR 2.13ActiveUS · Utility
Structure for inhibiting back end of line damage from dicing and chip packaging interaction failures
Inventors: Lane Michael W, Liu Xiao Hu, Shaw Thomas M, Farooq Mukta G, Hannon RobertAssignee: Lane Michael W, Liu Xiao HuFiled 2011-02-19 · Granted 2011-12-13

A semiconductor product comprises a semiconductor substrate having a top surface and a bottom surface including a semiconductor chip. The semiconductor substrate has a top surface and a perimeter. A barrier is formed in the chip within the perimeter. An Ultra Deep Isolation…

WO 2009/032488 A1#7248353 Most Cited · 13 citations0.8/yr · PR 4.40PendingWO · Application
Improved low k porous sicoh dielectric and integration with post film formation treatment

A porous SiCOH (e.g., p-SiCOH) dielectric film in which the stress change caused by increased tetrahedral strain is minimized by post treatment in unsaturated Hydrocarbon ambient. The inventive p-SiCOH dielectric film has more -(CHx) and less Si-O-H and Si-H bondings as compared…

US 2004126939 A1#10522729 Most Cited · 10 citations0.5/yr · PR 2.01PendingUS · Application
Gas treatment of thin film structures with catalytic action

A method of substantially reducing and/or eliminating the amount of defects and/or impurities that amass at interfacial surfaces that are present in a multilayer structure is provided. Specifically, the method improves the efficiency of a forming gas anneal by providing a…

US 2012329287 A1#11549793 Most Cited · 9 citations0.6/yr · PR 2.17PendingUS · Application
LOW k POROUS SiCOH DIELECTRIC AND INTEGRATION WITH POST FILM FORMATION TREATMENT

A porous SiCOH dielectric film in which the stress change caused by increased tetrahedral strain is minimized by post treatment in unsaturated Hydrocarbon ambient. The p-SiCOH dielectric film has more —(CHx) and less Si—O—H and Si—H bonding moieties. Moreover, a stable pSiOCH…

US 8,859,390 B2#11881513 Most Cited · 9 citations0.8/yr · PR 1.88ActiveUS · Utility
Structure and method for making crack stop for 3D integrated circuits

A structure to prevent propagation of a crack into the active region of a 3D integrated circuit, such as a crack initiated by a flaw at the periphery of a thinned substrate layer or a bonding layer, and methods of forming the same is disclosed.

US 8,242,600 B2#13949050 Most Cited · 8 citations0.6/yr · PR 1.43ActiveUS · Utility
Redundant metal barrier structure for interconnect applications
Inventors: Yang Chih-chao, Shaw Thomas MAssignee: Yang Chih-chao, Shaw Thomas MFiled 2009-05-19 · Granted 2012-08-14

A redundant metal diffusion barrier is provided for an interconnect structure which improves the reliability and extendibility of the interconnect structure. The redundant metal diffusion barrier layer is located within an opening that is located within a dielectric material and…

US 2005186689 A1#16385312 Most Cited · 6 citations0.3/yr · PR 2.98PendingUS · Application
Method and structure for determining thermal cycle reliability

A device and method for evaluating reliability of a semiconductor chip structure built by a manufacturing process includes a test structure built in accordance with a manufacturing process. The test structure is thermal cycled and the yield of the test structure is measured. The…

US 2014021622 A1#18810666 Most Cited · 6 citations0.5/yr · PR 1.26PendingUS · Application
Optimization metallization for prevention of dielectric cracking under controlled collapse chip connections

A method of reducing white bump formation and dielectric cracking under controlled collapse chip connections (C4s). The method comprises fabricating a substrate having a plurality of metallization layers, one or more of the layers is of low k dielectric material. The substrate…

US 8,592,306 B2#22369169 Most Cited · 5 citations0.4/yr · PR 1.16ActiveUS · Utility
Redundant metal barrier structure for interconnect applications
Inventors: Yang Chih-chao, Shaw Thomas MAssignee: Yang Chih-chao, Shaw Thomas MFiled 2012-06-21 · Granted 2013-11-26

A redundant metal diffusion barrier is provided for an interconnect structure which improves the reliability and extendibility of the interconnect structure. The redundant metal diffusion barrier layer is located within an opening that is located within a dielectric material and…

US 2005086628 A1#23073301 Most Cited · 4 citations0.2/yr · PR 1.89PendingUS · Application
Method of extracting properties of back end of line (BEOL) chip architecture

A method for analyzing circuit designs includes discretizing a design representation into pixel elements representative of a structure in the design and determining at least one property for each pixel element representing a portion of the design. Then, a response of the design…

US 2008224135 A1#23610919 Most Cited · 4 citations0.2/yr · PR 1.61PendingUS · Application
Method and structure for determining thermal cycle reliability

A device and method for evaluating reliability of a semiconductor chip structure built by a manufacturing process includes a test structure built in accordance with a manufacturing process. The test structure is thermal cycled and the yield of the test structure is measured. The…

US 8,362,596 B2#27209535 Most Cited · 4 citations0.3/yr · PR 1.08ActiveUS · Utility
Engineered interconnect dielectric caps having compressive stress and interconnect structures containing same
Inventors: Cohen Stephan A, Grill Alfred, Haigh Jr Thomas J, Liu Xiao H, Nguyen Son VAssignee: Ibm, Cohen Stephan AFiled 2009-07-14 · Granted 2013-01-29

A dielectric capping layer having a dielectric constant of less than 4.2 is provided that exhibits a higher mechanical and electrical stability to UV and/or E-Beam radiation as compared to conventional dielectric capping layers. Also, the dielectric capping layer maintains a…

US 2006273460 A1#34037815 Most Cited · 3 citations0.1/yr · PR 0.96PendingUS · Application
Method and structure for determining thermal cycle reliability

A device and method for evaluating reliability of a semiconductor chip structure built by a manufacturing process includes a test structure built in accordance with a manufacturing process. The test structure is thermal cycled and the yield of the test structure is measured. The…

US 2013049207 A1#30813025 Most Cited · 3 citations0.2/yr · PR 1.19PendingUS · Application
Multiple step anneal method and semiconductor formed by multiple step anneal

A method of annealing a semiconductor and a semiconductor. The method of annealing including heating the semiconductor to a first temperature for a first period of time sufficient to remove physically-adsorbed water from the semiconductor and heating the semiconductor to a…

US 2013270558 A1#34080801 Most Cited · 3 citations0.2/yr · PR 0.95PendingUS · Application
Semiconductor test and monitoring structure to detect boundaries of safe effective modulus

A method of testing an integrated circuit (IC) chip and a related test structure are disclosed. A test structure includes a monitor chain proximate to at least one solder bump pad, the monitor chain including at least one metal via stack, each metal via stack extending from a…

US 9,006,739 B2#34080804 Most Cited · 3 citations0.3/yr · PR 0.95ActiveUS · Utility
Semiconductor test and monitoring structure to detect boundaries of safe effective modulus

A method of testing an integrated circuit (IC) chip and a related test structure are disclosed. A test structure includes a monitor chain proximate to at least one solder bump pad, the monitor chain including at least one metal via stack, each metal via stack extending from a…

US 2005227380 A1#42511222 Most Cited · 2 citations0.1/yr · PR 0.95PendingUS · Application
Control of liner thickness for improving thermal cycle reliability

A device, system and method for evaluating reliability of a semiconductor chip are disclosed. Strain is determined at a location of interest in a structure. Failures are evaluated in a plurality of the structures after stress cycling to determine a strain threshold with respect…

US 2013345997 A1#42293429 Most Cited · 2 citations0.1/yr · PR 0.96PendingUS · Application
Integrated time dependent dielectric breakdown reliability testing

Methods for reliability testing include applying a stress voltage to a device under test (DUT); measuring a leakage current across the DUT; triggering measurement of optical emissions from the DUT based on the timing of the measurement of the leakage current; and correlating…

US 2014021616 A1#45095411 Most Cited · 2 citations0.2/yr · PR 0.88PendingUS · Application
Semiconductor structure

A semiconductor structure is provided and includes a substrate having an edge surface and a device surface with a central area, a crack stop structure disposed on the device surface and a circuit structure including components disposed on the device surface in the central area…

US 2014024146 A1#45401175 Most Cited · 2 citations0.2/yr · PR 0.86PendingUS · Application
Semiconductor structure

A semiconductor structure is provided and includes a substrate having an edge surface and a device surface with a central area, a crack stop structure disposed on the device surface and a circuit structure including components disposed on the device surface in the central area…

US 9,448,277 B2#45401056 Most Cited · 2 citations0.2/yr · PR 0.86ActiveUS · Utility
Integrated time dependent dielectric breakdown reliability testing
Inventors: Chen Jifeng, Pfeiffer Dirk, Shaw Thomas M, Song Peilin, Stellari FrancoAssignee: Chen Jifeng, Pfeiffer DirkFiled 2012-07-09 · Granted 2016-09-20

Systems for reliability testing include a picometer configured to measure a leakage current across a device under test (DUT); a camera configured to measure optical emissions from the DUT based on a timing of the measurement of the leakage current; and a test system configured…

US 2014207396 A1#45886088 Most Cited · 1 citations0.1/yr · PR 1.45PendingUS · Application
Integrated time dependent dielectric breakdown reliability testing

Systems for reliability testing include a picometer configured to measure a leakage current across a device under test (DUT); a camera configured to measure optical emissions from the DUT based on a timing of the measurement of the leakage current; and a test system configured…

US 9,018,089 B2#61066869 Most Cited · 1 citations0.1/yr · PR 0.75ActiveUS · Utility
Multiple step anneal method and semiconductor formed by multiple step anneal
Inventors: Liniger Eric G, Bonilla Griselda, Leung Pak, Cohen Stephen A, Gates Stephen MAssignee: Liniger Eric G, Bonilla GriseldaFiled 2011-08-30 · Granted 2015-04-28