Patents
US 2001023979 A1#2891734 Most Cited · 26 citations1.0/yr · PR 3.17PendingUS · Application
Method and system for dicing wafers, and semiconductor structures incorporating the products thereof

A method and system for dicing a semiconductor wafer providing a structure with greatly reduced backside chipping and cracking, as well as increased die strength. Semiconductor chip structures obtained from wafers diced according to this invention are also encompassed.

US 2004087078 A1#3212550 Most Cited · 24 citations1.1/yr · PR 4.11PendingUS · Application
Edge seal for a semiconductor device

An edge seal around the periphery of an integrated circuit device which environmentally protects the copper circuitry from cracks that may form in the low-k interlevel dielectric during dicing. The edge seal essentially constitutes a dielectric wall between the copper circuitry…

US 2003211707 A1#6270193 Most Cited · 15 citations0.7/yr · PR 2.87PendingUS · Application
Method and system for dicing wafers, and semiconductor structures incorporating the products thereof

A method and system for dicing a semiconductor wafer providing a structure with greatly reduced backside chipping and cracking, as well as increased die strength. Semiconductor chip structures obtained from wafers diced according to this invention are also encompassed.

US 2013049207 A1#30813025 Most Cited · 3 citations0.2/yr · PR 1.19PendingUS · Application
Multiple step anneal method and semiconductor formed by multiple step anneal

A method of annealing a semiconductor and a semiconductor. The method of annealing including heating the semiconductor to a first temperature for a first period of time sufficient to remove physically-adsorbed water from the semiconductor and heating the semiconductor to a…

US 9,018,089 B2#61066869 Most Cited · 1 citations0.1/yr · PR 0.75ActiveUS · Utility
Multiple step anneal method and semiconductor formed by multiple step anneal
Inventors: Liniger Eric G, Bonilla Griselda, Leung Pak, Cohen Stephen A, Gates Stephen MAssignee: Liniger Eric G, Bonilla GriseldaFiled 2011-08-30 · Granted 2015-04-28

A method of annealing a semiconductor and a semiconductor. The method of annealing including heating the semiconductor to a first temperature for a first period of time sufficient to remove physically-adsorbed water from the semiconductor and heating the semiconductor to a…

WO 2006/096813 A2#47390228 Most Cited · 1 citations0.1/yr · PR 0.97PendingWO · Application
Low k dielectric cvd film formation process with in-situ imbedded nanolayers to improve mechanical properties

A material stack (12) is provided comprising one or more films (14) that have a crack velocity of about IE- 10 m/sec or greater and at least one monolayer (16) within or in direct contact with the one or more films (14), wherein the at least one monolayer (16) reduces the crack…

WO 2007/089223 A2#50586499 Most Cited · 1 citations0.1/yr · PR 0.85PendingWO · Application
Ultralow dielectric constant layer with controlled biaxial stress

A method for forming a ultralow dielectric constant layer with controlled biaxial stress is described incorporating the steps of forming a layer containing Si, C, O and H by one of PECVD and spin-on coating and curing the film in an environment containing very low concentrations…

WO 2004/042817 A1#127986343 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method and structure to enhance temperature/humidity/bias performance of semiconductor devices by surface modification

A method is disclosed of repairing wirebond damage on semiconductor chips such as high speed semiconductor microprocessors, application specific integrated circuits (ASICs), and other high speed integrated circuit devices, particularly devices using low-k dielectric materials.…

WO 2006/096813 A3#141808089 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Low k dielectric cvd film formation process with in-situ imbedded nanolayers to improve mechanical properties

A material stack (12) is provided comprising one or more films (14) that have a crack velocity of about IE- 10 m/sec or greater and at least one monolayer (16) within or in direct contact with the one or more films (14), wherein the at least one monolayer (16) reduces the crack…

WO 2007/089223 A3#129600025 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Ultralow dielectric constant layer with controlled biaxial stress

A method for forming a ultralow dielectric constant layer with controlled biaxial stress is described incorporating the steps of forming a layer containing Si, C, O and H by one of PECVD and spin-on coating and curing the film in an environment containing very low concentrations…