A method and apparatus for measuring the concentration of mobile ions in the oxide layer of a semiconductor wafer from the contact potential shift caused by ion drift across the oxide that includes depositing charge (e.g., using a corona discharge device) on the surface of the…
Semiconductor Diagnostics Inc
SILC characteristics and density of GOI defects of silicon wafers with thin dielectric films (e.g. SiO 2 ) are determined using a non-contact method that does not require any test structures on the wafer. The method includes stressing a dielectric with a corona discharge and…
A method of determining charge associated with traps present in a semiconductor oxide interface is described. The method includes the steps of depositing a dose of charge over a surface of the oxide and measuring a resultant value of surface potential barrier at the portion of…
A method is described for non-contact measuring the capacitance and the equivalent oxide thickness of ultra thin dielectric layer on a silicon substrate. The surface of a dielectric layer is electrically charged by a flux on ions from a corona discharge source until a steady…
The invention relates to a device for contacting and electrically grounding semiconductor substrate coated with or otherwise having an insulating film positioned thereover. The device includes a chuck having a wafer support surface which holds the wafer and a scriber movably…
Minority carrier diffusion lengths are determined fast, accurately, and conveniently by illuminating a surface of the semiconductor with a beam composed of a plurality of light fluxes each having a different wavelength modulated at a different frequency. Surface photovoltages…
A non-contact method is described for acquiring the accurate charge-voltage data on miniature test sites of semiconductor wafer wherein the test sites are smaller than 100 μm times 100 μm. The method includes recognizing the designated test site, properly aligning it, depositing…
A method and apparatus for measuring the concentration of different mobile ions in the oxide layer of a semiconductor wafer from the contact potential shift caused by different ions drifting across the oxide that includes depositing charge (e.g., using a corona discharge device)…
A method is described for measuring the capacitance and the equivalent oxide thickness of an ultra thin dielectric layer on a silicon substrate in which the dielectric layer is uniform or patterned. The surface of a dielectric layer is electrically charged by a flux on ions from…
Minority carrier diffusion lengths are determined fast, accurately, and conveniently by illuminating a surface of the semiconductor wafer (8) with a beam (7) composed of a plurality of light fluxes each having a different wavelength modulated at a different frequency (f1, f2).…
Techniques for determining the composition of mixed dielectric layers are disclosed.
A method is described for measuring the capacitance and the equivalent oxide thickness of an ultra thin dielectric layer (13a) on a silicon (11) substrate in which the dielectric layer is uniform or patterned. The surface (15) of a dielectric layer is electrically charged by a…
Techniques for measuring a contact potential difference of a sample at an elevated temperature using a probe designed for room temperature measurement are disclosed. In such measurements, probe damage by excessive heating can be prevented without any probe modifications to…
Minority carrier diffusion lengths are determined fast, accurately, and conveniently by illuminating a surface of the semiconductor wafer (8) with a beam (7) composed of a plurality of light fluxes each having a different wavelength modulated at a different frequency (f1, f2).…
Surface photo-voltage measurements are used to accurately determine very long steady state diffusion length of minority carriers and to determine iron contaminant concentrations and other recombination centers in very pure wafers. Disclosed methods use multiple (e.g., at least…
The surface photovoltage dopant concentration measurement of a semiconductor wafer is calibrated by biasing the semiconductor wafer into an avalanche breakdown condition in a surface depletion region; determining a contact potential difference value corresponding to an avalanche…
SILC characteristics and density of GOI defects of silicon wafers with thin dielectric films (e.g. SiO2) are determined using a non-contact method that does not require any test structures on the wafer. The method includes stressing a dielectric with a corona discharge and…
SILC characteristics and density of GOI defects of silicon wafers with thin dielectric films (e.g. SiO2) are determined using a non-contact method that does not require any test structures on the wafer. The method includes stressing a dielectric with a corona discharge and…
SILC characteristics and density of GOI defects of silicon wafers with thin dielectric films (e.g. SiO2) are determined using a non-contact method that does not require any test structures on the wafer. The method includes stressing a dielectric with a corona discharge and…
The invention relates to a device for contacting and electrically grounding semiconductor substrate coated with or otherwise having an insulating film positioned thereover. The device includes a chuck (10) having a wafer (12) support surface which holds the wafer (12) and a…