This invention relates to the measurement of the minority carrier diffusion length of a semiconductor sample to evaluate the contaminant impurities which reduce the carrier lifetime.
Lagowski; Jacek
A device for measuring photoinduced electrical properties at a semiconductor sample surface. The device includes an analysis probe having a means for directing a light beam to a defined portion of a semiconductor substrate surface. A probe electrode is provided for detecting a…
A method for determining the depletion layer minority carrier lifetime τ o in a depletion layer of a semiconductor wafer includes the following. A depletion layer is induced on a surface of the wafer. The wafer is heated to a temperature T 1 . A surface photovoltage is induced…
A non-contact method is described for acquiring the accurate charge-voltage data on miniature test sites of semiconductor wafer wherein the test sites are smaller than 100 μm times 100 μm. The method includes recognizing the designated test site, properly aligning it, depositing…
Minority carrier diffusion lengths are determined fast, accurately, and conveniently by illuminating a surface of the semiconductor wafer (8) with a beam (7) composed of a plurality of light fluxes each having a different wavelength modulated at a different frequency (f1, f2).…
Surface photo-voltage measurements are used to accurately determine very long steady state diffusion length of minority carriers and to determine iron contaminant concentrations and other recombination centers in very pure wafers. Disclosed methods use multiple (e.g., at least…
Techniques for measuring a contact potential difference of a sample at an elevated temperature using a probe designed for room temperature measurement are disclosed. In such measurements, probe damage by excessive heating can be prevented without any probe modifications to…
A method is described for measuring the capacitance and the equivalent oxide thickness of an ultra thin dielectric layer (13a) on a silicon (11) substrate in which the dielectric layer is uniform or patterned. The surface (15) of a dielectric layer is electrically charged by a…
Methods of measuring copper impurities on a silicon surface are disclosed. In certain embodiments, copper is electrically activated by ultra-violet illumination of the surface at room temperature. Activation can enhance the copper contribution to surface recombination and to…
Surface photo-voltage measurements are used to accurately determine very long steady state diffusion length of minority carriers and to determine iron contaminant concentrations and other recombination centers in very pure wafers. Disclosed methods use multiple (e.g., at least…
SILC characteristics and density of GOI defects of silicon wafers with thin dielectric films (e.g. SiO2) are determined using a non-contact method that does not require any test structures on the wafer. The method includes stressing a dielectric with a corona discharge and…
The invention relates to a device for contacting and electrically grounding semiconductor substrate coated with or otherwise having an insulating film positioned thereover. The device includes a chuck (10) having a wafer (12) support surface which holds the wafer (12) and a…
SILC characteristics and density of GOI defects of silicon wafers with thin dielectric films (e.g. SiO2) are determined using a non-contact method that does not require any test structures on the wafer. The method includes stressing a dielectric with a corona discharge and…
Methods of measuring copper impurities on a silicon surface are disclosed. In certain embodiments, copper is electrically activated by ultra-violet illumination of the surface at room temperature. Activation can enhance the copper contribution to surface recombination and to…