US 2009215605 A1#3950252 Most Cited · 21 citations1.2/yr · PR 3.35PendingUS · Application
Process of producing a glass-ceramic, the glass-ceramic made therby and its uses

The process of making the glass-ceramic includes ceramicizing a starting glass at a heating or cooling rate during the ceramicization of at least 10 K/min, so that the glass-ceramic contains at least 50% by volume of ferroelectric crystallites with a maximum diameter of from 20…

US 8,141,387 B2#8436996 Most Cited · 12 citations0.9/yr · PR 2.27ActiveUS · Utility
Process of producing a glass-ceramic, the glass-ceramic made therby and its uses
Inventors: Letz Martin, Davis Mark J, Ruedinger Bernd, Hoppe Bernd, Schreder BiancaAssignee: Letz Martin, Davis Mark JFiled 2009-02-25 · Granted 2012-03-27

The process of making the glass-ceramic includes ceramicizing a starting glass at a heating or cooling rate during the ceramicization of at least 10 K/min, so that the glass-ceramic contains at least 50% by volume of ferroelectric crystallites with a maximum diameter of from 20…

WO 2012/034648 A1#8498719 Most Cited · 12 citations0.9/yr · PR 2.15PendingWO · Application
Syringe body/needle assembly and method for producing same

The invention relates to a syringe body/needle assembly (10, 20, 30) and to a method for producing such a syringe body/needle assembly. By means of the invention, a syringe body/needle assembly is produced, in which an adhesive bond by means of organic adhesive is dispensed with.

US 2011028298 A1#10314245 Most Cited · 10 citations0.7/yr · PR 2.25PendingUS · Application
Glass-ceramic containing nanoscale barium titanate and process for the production thereof

A process for the production of a glass-ceramic comprises the following steps: a) providing a mixture comprising at least SiO 2 , Al 2 O 3 , BaO and TiO 2 , b) melting the mixture in order to produce a glass phase, c) cooling the glass phase, and d) ceramicizing the glass phase.…

US 2013231617 A1#12186638 Most Cited · 9 citations0.7/yr · PR 1.58PendingUS · Application
Syringe body/needle assembly and method for producing same

A syringe body/needle assembly and a method for producing such a syringe body/needle assembly are provided that if free of an organic adhesive bond.

US 2013120193 A1#18391962 Most Cited · 6 citations0.5/yr · PR 1.44PendingUS · Application
Glass ceramics for use as a dielectric for gigahertz applications

A glass-ceramic which is particularly suitable as dielectric for use in the high-frequency range, in particular as dielectric resonator, as electronic frequency filter element or as antenna element is disclosed. The glass-ceramic has at least the following constituents (in mol %…

US 2013237400 A1#17880806 Most Cited · 6 citations0.5/yr · PR 1.58PendingUS · Application
Glass-ceramic having at least two crystal phases, process for producing a glass-ceramic and its use

A glass-ceramic having at least two crystal phases, wherein at least one crystal phase has a positive temperature dependence of the resonance frequency τ f , at least one crystal phase has a negative temperature dependence of the resonance frequency τ f and the glass-ceramic has…

US 8,772,188 B2#33057071 Most Cited · 3 citations0.2/yr · PR 1.06ActiveUS · Utility
Glass-ceramic having at least two crystal phases, process for producing a glass-ceramic and its use
Inventors: Letz Martin, Knoener Stephan, Dressler Martina, Seiler Daniela, Hoppe BerndAssignee: Letz Martin, Knoener StephanFiled 2012-03-12 · Granted 2014-07-08

A glass-ceramic having at least two crystal phases, wherein at least one crystal phase has a positive temperature dependence of the resonance frequency τ f , at least one crystal phase has a negative temperature dependence of the resonance frequency τ f and the glass-ceramic has…

WO 02,083,586 A1#36388278 Most Cited · 2 citations0.1/yr · PR 1.17PendingWO · Application
Method for reducing the adhesion tendency during the hot forming of glass

The invention relates to a method and a device for reducing the adhesion tendency during the hot forming of a glass body, using at least two moulds, which are positioned on either side of the glass body and are brought into contact with the glass body at a temperature, at which…

US 8,263,509 B2#50448219 Most Cited · 1 citations0.1/yr · PR 0.85ActiveUS · Utility
Glass-ceramic containing nanoscale barium titanate and process for the production thereof
Inventors: Hoppe Bernd, Seiler Daniela, Ruedinger Bernd, Mitra Ina, Reich Maria-louisaAssignee: Hoppe Bernd, Seiler DanielaFiled 2010-06-04 · Granted 2012-09-11

A process for the production of a glass-ceramic comprises the following steps: a) providing a mixture comprising at least SiO2, Al2O3, BaO and TiO2, b) melting the mixture in order to produce a glass phase, c) cooling the glass phase, and d) ceramicizing the glass phase. In the…

WO 03,014,037 A1#49074484 Most Cited · 1 citations0.0/yr · PR 0.89PendingWO · Application
Method and device for detecting imminent surface adhesion between a glass body to be formed and a form tool

The invention relates to a method for detecting imminent surface adhesion during a forming process, between a glass body (3) to be formed and at least two electroconductive tools (2a, 2b) arranged on both sides of the glass body (3), in a temperature range in which the glass…

US 8,998,853 B2#142012784 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Syringe body/needle assembly and method for producing same
Inventors: Hoppe Bernd, Seiler Daniela, Roters Andreas, Schellenberg KatrinAssignee: Hoppe Bernd, Seiler DanielaFiled 2011-08-30 · Granted 2015-04-07

A syringe body/needle assembly and a method for producing such a syringe body/needle assembly are provided that if free of an organic adhesive bond.

WO 2012/034648 A9#111528309 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Syringe body/needle assembly and method for producing same

The invention relates to a syringe body/needle assembly (10, 20, 30) and to a method for producing such a syringe body/needle assembly. By means of the invention, a syringe body/needle assembly is produced, in which an adhesive bond by means of organic adhesive is dispensed with.

WO 2013/076114 A2#86924972 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Glass-ceramic as dielectric in the high-frequency range

A glass-ceramic which can in particular be used as dielectric and has at least the following constituents (in mol% on an oxide basis): SiO 2 1 - 50, Al 2 O 3 0 - 20, B 2 O 3 0 - 25, TiO 2 10 - 70, RE 2 O 3 0 - 35, BaO 0 - 35, where RE is lanthanum, another lanthanide or yttrium…

WO 2013/076114 A3#129727247 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Glass-ceramic as dielectric in the high-frequency range

A glass-ceramic which can in particular be used as dielectric and has at least the following constituents (in mol% on an oxide basis): SiO 2 1 - 50, Al 2 O 3 0 - 20, B 2 O 3 0 - 25, TiO 2 10 - 70, RE 2 O 3 0 - 35, BaO 0 - 35, where RE is lanthanum, another lanthanide or yttrium…