Abstract

A glass-ceramic having at least two crystal phases, wherein at least one crystal phase has a positive temperature dependence of the resonance frequency τ f , at least one crystal phase has a negative temperature dependence of the resonance frequency τ f and the glass-ceramic has a resulting temperature dependence of the resonance frequency τ f of 0 ppm/K with a maximum deviation of +/−20 ppm/K, is described. Furthermore, a process for producing such a glass-ceramic and the use of the glass-ceramic are described.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 3.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A glass-ceramic having at least two crystal phases, wherein at least one crystal phase has a positive temperature dependence of the resonance frequency τ f , at least one crystal phase has a negative temperature dependence of the resonance frequency τ f and the glass-ceramic has a resulting temperature dependence of the resonance frequency τ f of 0+/−20 ppm/K, and wherein the glass-ceramic has at least the following constituents (in mol % on an oxide basis): SiO 2 5-50 Al 2 O 3 0-20

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Non-Patent Literature (5)

  • English Translation of Office Action dated Apr. 1, 2011 corresponding to German Patent Application No. 102010032982.7-45.
  • Mirsaneh, M., et al., "Circularly Polarized Dielectric-Loaded Antennas: Current Technology and Future Challenges," Adv. Funct. Mater., 2008, 18, pp. 1-8.
  • Office Action dated Apr. 1, 2011 corresponding to German Patent Application No. 102010032982.7-45.
  • Sebastian, M. T., et al., "Low loss dielectric materials for LTCC applications: a review;" 2008 Institute of Materials, Minerals and Mining and ASM International, 2008, vol. 53, No. 3, pp. 57-90.
  • Takahashi, J., et al., "Microwave Deilectric Properties of Lanthanide Titanate Ceramics," Jpn. J. Appl. Phys., vol. 32 (1993), pp. 4327-4331, Part 1, No. 9B, Sep. 1993.