Ni and Pt residuals are eliminated by replacing an SPM cleaning process with application of HNO 3 in an SWC tool. Embodiments include depositing a layer of Ni/Pt on a semiconductor substrate, annealing the deposited Ni/Pt layer, removing unreacted Ni from the annealed Ni/Pt…
Poth Jochen
The amount of Pt residues remaining after forming Pt-containing NiSi is reduced by performing a rework including applying SPM at a temperature of 130° C. in a SWC tool, if Pt residue is detected. Embodiments include depositing a layer of Ni/Pt on a semiconductor substrate,…
The amount of Pt residues remaining after forming Pt-containing NiSi is reduced by performing a rework including applying SPM at a temperature of 130° C. in a SWC tool, if Pt residue is detected. Embodiments include depositing a layer of Ni/Pt on a semiconductor substrate,…
Ni and Pt residuals are eliminated by replacing an SPM cleaning process with application of HNO 3 in an SWC tool. Embodiments include depositing a layer of Ni/Pt on a semiconductor substrate, annealing the deposited Ni/Pt layer, removing unreacted Ni from the annealed Ni/Pt…