Abstract

Ni and Pt residuals are eliminated by replacing an SPM cleaning process with application of HNO 3 in an SWC tool. Embodiments include depositing a layer of Ni/Pt on a semiconductor substrate, annealing the deposited Ni/Pt layer, removing unreacted Ni from the annealed Ni/Pt layer by applying HNO 3 to the annealed Ni/Pt layer in an SWC tool, annealing the Ni removed Ni/Pt layer, and removing unreacted Pt from the annealed Ni removed Ni/Pt layer. Embodiments include forming first and second gate electrodes on a substrate, spacers on opposite sides of each gate electrode, and Pt-containing NiSi on the substrate adjacent each spacer, etching back the spacers, forming a tensile strain layer over the first gate electrode, applying a first HNO 3 in an SWC tool, forming a compressive strain layer over the second gate electrode, and applying a second HNO 3 in an SWC tool.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method comprising: depositing a layer of nickel (Ni)/platinum (Pt) on a semiconductor substrate; annealing the deposited Ni/Pt layer; removing unreacted Ni from the annealed Ni/Pt layer by applying nitric acid (HNO3) to the annealed Ni/Pt layer in a single wafer clean (SWC) tool; annealing the Ni removed Ni/Pt layer; removing unreacted Pt from the annealed Ni removed Ni/Pt layer; and performing an SC1 spray process subsequent to applying HNO3 to the annealed Ni/Pt layer and prior to annealing the Ni removed Ni/Pt layer.

  2. Claim 2Depends on #1

    The method according to claim 1 , comprising applying HNO3 to the annealed Ni/Pt layer at a volume ratio of HNO3 to water of 1:1 or 1:20.

  3. Claim 3Depends on #2

    The method according to claim 2 , comprising applying HNO3 to the annealed Ni/Pt layer at a temperature of 40° C. to 60° C.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.