Heat treatment of alloys having elements for improving grain boundary strength. Components directly after castings often reveal a low or no transverse grain boundary strength, so that cracks do appear and decrease the yield rate. The inventive measures does not lead to low…
Pickert Ursula
Heat treatment of alloys having elements for improving grain boundary strength is disclosed. Components directly after castings often reveal low or no transverse grain boundary strength, so that cracks do appear and decrease the yield rate. The provided measures do not lead to…
A nickel-based superalloy is provided. Known nickel-based superalloys for producing components made of stem shaped single crystals do not provide sufficiently for grain boundary strength. The superalloy includes a low molybdenum content and very accurately adjusted values for…
Heat treatment of alloys having elements for improving grain boundary strength Components directly after castings often reveal a low or no transverse grain boundary strength, so that cracks do appear and decrease the yield rate. The inventive measures does not lead to low…
The invention relates to a method for repairing components (1) comprising a base material with an oriented microstructure, wherein the repair point (3) comprises a correspondingly oriented microstructure as the surrounding base material. According to the inventive method, solder…
Plastics do not have the mechanical or erosive properties required for specific areas of application. The inventive plastic comprising powder particles (7) improves the properties of said plastic in relation to mechanical characteristics and erosive properties for components,…
A method of producing a component wherein a directionally solidified columnar grained cast superalloy material is heat treated such that a secondary phase of the alloy is only partly solved, thereby providing improved transverse stress rupture strength compared to fully solved…
The invention relates to a blade (1) for a turbine engine (41) with a base body (2), made from a titanium alloy, with a first and a second component piece (11,13), which are connected in a connection region (31) by means of a bonding process. A groove (23) with a groove wall…
The invention relates to a method for the production of a pattern for precision casting representation of a turbine component comprising at least one cavity, whereby the prepared pattern comprises at least one core and an outer contour pattern (1), at least partly enclosing the…
Plastics do not have the mechanical or erosive properties required for specific areas of application. The inventive plastic comprising powder particles (7) improves the properties of said plastic in relation to mechanical characteristics and erosive properties for components,…
Plastics do not have the mechanical or erosive properties required for specific areas of application. The inventive plastic comprising powder particles (7) improves the properties of said plastic in relation to mechanical characteristics and erosive properties for components,…