The present invention relates to a high-temperature part (1) made of a nickel super-alloy having the following composition in wt %: 11-13 % of Cr; 3-5 % of W; 0.5-2.5 % of Mo; 3-5 % of Al; 3-5 % of Ti; 3-7 % of Ta; 1-5 % of Re; the balance consisting of nickel. This invention…
Esser Winfried
Component repair process, in which a loss of wall thickness is repaired just by a standard coating, results in a component with a layer which has properties that are less than optimum in the repaired region at elevated temperatures. The process according to the invention…
A casting mold for a metal melt is provided. By coating a core of a casting mold, the core may be mechanically stabilized and an inner coating of the component to be cast may be obtained, wherein the coating preferably serves as an anti-corrosion layer. A method for producing a…
The invention relates to a turbine blade (1) which extends along a principal axis (2) of a foot area (3) up to a head area (5) via a blade area (4). A feed (6) for cooling liquid (16) is provided in the blade area (4), said feed being surrounded by a thin outerwall (7) of the…
A turbine blade for a turbine of a thermal power plant, with a platform for partial delimiting of a flow passage in the turbine, wherein the platform has at least one cooling medium passage, which extends inside the platform, for guiding a cooling medium, is characterized…
The invention a high temperature resistant component made of an alloy, in particular a nickel-based-super alloy in the following composition and expressed in weight percentage: 9-13% Cr, 3-5% W, 0.5-2.5% Mo, 3-5% Ti, 3-7% Ta, 1-5% Re, up to 2000 ppm of a solidification promoter,…
Heat treatment of alloys having elements for improving grain boundary strength. Components directly after castings often reveal a low or no transverse grain boundary strength, so that cracks do appear and decrease the yield rate. The inventive measures does not lead to low…
This invention concerns a process for directed solidification of a melt (1) of an alloy containing a basic metal in a mould (2, 3), wherein the mould (2, 3) filled with the melt (1) is introduced into a cooling bath (4) to effect solidification of the melt (1). A metal sheet (5)…
A rotor blade system, for example, of a gas turbine is provided. The rotor blade system includes a plurality of rotor blades which are arranged annularly on a rotor disk. A plurality of sealing plates are arranged on a side surface of the rotor disk. An individual sealing plate…
The invention relates to a guide blade segment of a thermal turbomachine, in particular a gas turbine, comprising a number of profiled blades which are arranged on a platform. A plurality of securing elements for securing the guide blade segment to an associated guide blade…
A guide vane for a gas turbine with a vane base body which is of single-piece design and comprises a profiled vane blade extending between a vane root and a cover plate and also the vane root formed integrally with the vane blade and the cover plate formed integrally with the…
The invention a high temperature resistant component made of an alloy, in particular a nickel-based-super alloy in the following composition and expressed in weight percentage: 9-13 % Cr, 3-5 % W, 0,5-2,5 % Mo, 3-5 % Al, 3-5 % Ti, 3-7 % Ta, 1-5 % Re, upto 2000 ppm of a…
A nickel-based superalloy is provided. Known nickel-based superalloys for producing components made of stem shaped single crystals do not provide sufficiently for grain boundary strength. The superalloy includes a low molybdenum content and very accurately adjusted values for…
A layer system including a substrate and a layer is provided. The layer system has a hole at least in the layer, and wherein at least one recess is present in a surface of the layer in a vicinity around the hole or directly adjoining a boundary line of the hole.
Heat treatment of alloys having elements for improving grain boundary strength is disclosed. Components directly after castings often reveal low or no transverse grain boundary strength, so that cracks do appear and decrease the yield rate. The provided measures do not lead to…
Directionally solidified columnar grain nickel base alloy casting consisting essentially of, in weight %, of about 11.6% to 12.70% Cr, about 8.50 to 9.5% Co, about 1.65% to 2.15% Mo, about 3.5% to 4.10% W, about 4.80% to 5.20% Ta, about 3.40 to 3.80% Al, about 3.9% to 4.25% Ti,…
A core die is provided. The core die includes a first half and a second half where a cavity is formed between the two. Pins are arranged on the halves and the pins are replaceable. By virtue of the modular inner structure of a core die, the core die may be matched to the desired…
A method to produce a metallic component is described. The method provides that an additional shot peening is performed on at least portion of component in order to obtain a fine grain structure during a following heat treatment in order to yield higher HCF because a finer grain…
The invention relates to a turbine blade (1), especially a gas turbine blade. The inventive turbine blade extends along a main axis (2) from a base area (3) to a top area (5), via a flat blade area (4). The blade has a hollow space (6) in the area of the flat blade part (4)…
Heat treatment of alloys having elements for improving grain boundary strength Components directly after castings often reveal a low or no transverse grain boundary strength, so that cracks do appear and decrease the yield rate. The inventive measures does not lead to low…
During a solution heat treatment grain recrystallization may occur of a textured article, especially at the surface rim. The present invention provides a method for restoring the microstructure of a textured article, which comprises coating the surface of the article with a high…
Known nickel-based super alloys for producing components made of stem-shaped single crystals do not provide sufficiently for grain boundary strength. The proposed nickel-based super alloy has a low molybdenum content and very accurately adjusted values for elements having grain…
The invention relates to a process for removing tin from a surface and/or the region close to the surface of a component in which the component is subjected to a flow of concentrated caustic soda or hydrochloric acid at a temperature considerably above ambient temperature. The…
There is described a turbine blade with an aerodynamically profiled blade leaf which is produced from two assembled shell elements. The shell elements forming the suction-side and the pressure-side blade leaf wall have been assembled by means of a high-temperature high-pressure…