Patents
Assignee / Organization

Mcdonald Stuart David

16Total Forward Citations
6Indexed Patents
3Avg Citations / Patent
3Portfolio H-Index
WO 2013/002112 A1#16722166 Most Cited · 6 citations0.5/yr · PR 2.15PendingWO · Application
Process for producing solder joint with improved reliability

A highly reliable joint which is inhibited, during operation, from suffering a volume change accompanying phase transformation or suffering troubles such as strains or cracks caused by a volume change is rendered possible with an Sn-Cu solder alloy by regulating the cooling…

US 2014030140 A1#33810940 Most Cited · 3 citations0.2/yr · PR 1.00PendingUS · Application
Solder alloy

A solder alloy may include a Sn—Cu hypereutectic area having Cu in the amount of up to 7.6 weight percent, from 0.006 to 0.5 weight percent of Al, Al 2 O 3 , or a combination thereof.

WO 2006/058388 A1#32240690 Most Cited · 3 citations0.1/yr · PR 1.11PendingWO · Application
Aluminium casting alloy

A method of forming a hypoeutectic aluminium silicon alloy including the steps of: forming an aluminium melt including greater than zero and less than about 12 wt% silicon, adding 20-3000 ppm of a eutectic modifying element selected from the group consisting of strontium,…

WO 2012/137901 A1#39864129 Most Cited · 2 citations0.1/yr · PR 1.02PendingWO · Application
Solder alloy

This solder alloy contains Al and/or Al 2 O 3 in the amount of 0.006-0.15 wt% in an Sn-Cu hypereutectic area. In addition, this solder alloy comprises Cu in the amount of 0.7-7.6 wt%, and Al and/or Al 2 O 3 in the amount of 0.006-0.5 wt%, with the remainder being Sn. Preferably,…

US 8,097,101 B2#61578667 Most Cited · 1 citations0.1/yr · PR 0.75ExpiredUS · Utility
Aluminium casting alloy
Inventors: Dahle Arne Kristian, Lu Liming, Nogita Kazuhiro, Mcdonald Stuart DavidAssignee: Dahle Arne Kristian, Lu LimingFiled 2005-12-02 · Granted 2012-01-17

A method of forming a hypoeutectic aluminium silicon alloy including the steps of: forming an aluminium melt including greater than zero and less than about 12 wt % silicon, adding 20-3000 ppm of a eutectic modifying element selected from the group consisting of strontium,…

US 9,999,945 B2#61548769 Most Cited · 1 citations0.1/yr · PR 0.75ActiveUS · Utility
Solder alloy

A solder alloy may include a Sn—Cu hypereutectic area having Cu in the amount of up to 7.6 weight percent, from 0.006 to 0.5 weight percent of Al, Al 2 O 3 , or a combination thereof.