An aluminosilicate glass article having a high compressive stress layer. The glass article comprises at least about 50 mol % SiO 2 and at least about 11 mol % Na 2 O, and has a layer under a compressive stress of at least about 900 MPa and the depth of layer that extends at…
Mauro John
The described embodiments may provide a method of fabricating a chemical detection device. The method may comprise forming a microwell above a CMOS device. The microwell may comprise a bottom surface and sidewalls. The method may further comprise applying a first chemical to be…
Glass compositions and glass articles comprising the glass compositions are disclosed. In one embodiment, a glass composition includes from about 65 mol.% to about 70 mol.% SiO2; from about 9 mol.% to about 14 mol.% Al 2 O 3 ; and from about 0 mol.% to about 11 mol.% B 2 O 3 as…
Glass compositions that may be used to produce chemically strengthened glass sheets by ion exchange. The glass compositions are chosen to promote simultaneously high compressive stress and deep depth of layer or, alternatively, to reduce the time needed to ion exchange the glass…
A glass article including at least about 40 mol % SiO 2 and, optionally, a colorant imparting a preselected color is disclosed. In general, the glass includes, in mol %, from about 40-70 SiO 2 , 0-25 Al 2 O 3 , 0-10 B 2 O 3 ; 5-35 Na 2 O, 0-2.5 K 2 O, 0-8.5 MgO, 0-2 ZnO, 0-10% P…
Described herein are alkali-free, boroalumino silicate glasses exhibiting desirable physical and chemical properties for use as substrates in flat panel display devices, such as, active matrix liquid crystal displays (AMLCDs) and active matrix organic light emitting diode…
A device ( 16 ) in a system ( 10 ) modulates an optical signal ( 13 ) and tunes the duty cycle of the optical signal ( 13 ) for optimizing system performance as a response of the duty cycle. The device ( 16 ) includes a tunable duty-cycle Mach-Zehnder interferometer (MZI) acting…
Low CTE glass compositions and glass articles formed from the same are described. In one embodiment, a glass composition includes from about 60 mol.% to about 66 mol.% SiO 2 ; from about 7 mol.% to about 10 mol.% AI 2 O 3 ; and from about 14 mol.% to about 18 mol.% B 2 O 3 as…
Described herein are alkali-free, boroalumino silicate glasses exhibiting desirable physical and chemical properties for use as substrates in flat panel display devices, such as, active matrix liquid crystal displays (AMLCDs) and active matrix organic light emitting diode…
Glasses that can be chemically strengthened and are colored by transition metals. Most of the glasses are black, with some having high damage resistance and compressive surface layers having high compressive stress and depth of layer after ion exchange. These colored glasses do…
Provided herein are methods for making water-soluble nanoparticles comprising a core/shell nanocrystal that is coated with a surface layer comprising enough hydrophilic ligands to render the nanoparticle water soluble or water dispersable. Methods for crosslinking molecules on…
An aluminosilicate glass article having a high compressive stress layer. The glass article comprises at least about 50 mol % SiO 2 and at least about 11 mol % Na 2 O, and has a layer under a compressive stress of at least about 900 MPa and the depth of layer that extends at…
An optical transmitter ( 8 ) having enhanced stimulated Brillouin scattering (SBS) threshold power (PSBS) capability is disclosed. The transmitter includes a light source ( 12 ) adapted to emit a continuous-wave (CW) light beam ( 16 ). A phase modulator ( 20 ) is optically…
An aluminosilicate glass article having a high compressive stress layer. The glass article comprises at least about 50 mol% SiO 2 and at least about 11 I mol% Na 2 0, and has a layer under a compressive stress of at least about 900 MPa and the depth of layer that extends at…
High CTE glass compositions and laminated glass articles formed from the same are described. In one embodiment, a glass composition may include from about 70 mol.% to about 80 mol.% SiO 2 , from about 0 mol.% to about 8 mol.% Al 2 O 3 , and from about 3 mol.% to about 10 mol.% B…
Methods are provided for reducing the dimensional changes of a glass substrate during a display manufacturing process. The reductions are achieved by increasing the fast relaxation exhibited by the glass. Test methods are provided for distinguishing the effects on dimensional…
A nanoparticle having one or more phosphonates or phosphinate ligands on their surface can be converted into nanoparticles with sulfonate ligands on their surface, by contacting the phosphonate-containing nanoparticles with a silylsulfonate reagent. Such nanoparticles are…
Silicate glasses that are fictivated and fast cooled and have high levels of intrinsic or "native" damage resistance. When ion exchanged, the silicate glasses described herein have a Vickers crack initiation threshold of at least 15 kgf and, in some embodiments, at least…
The described embodiments may provide a method of fabricating a chemical detection device. The method may comprise forming a microwell above a CMOS device. The microwell may comprise a bottom surface and sidewalls, The method may further comprise applying a first chemical to be…
A compositional range of high strain point and/or intermediate expansion coefficient alkali metal free aluminosilicate and boroaluminosilicate glasses are described herein. The glasses can be used as substrates or superstrates for photovoltaic devices, for example, thin film…
Methods and apparatus for predicting viscosities of glass materials as a function of temperature and composition are provided. Two fitting parameters (fitting coefficients) are used for each of the viscosity-affecting components contained in the material. The parameters can…
Provided are reagents and methods for non-invasive in vivo imaging wherein the reagents comprise targeted carrier molecules conjugated to a NIR reporter molecule. In one aspect the targeted carrier molecule is an antibody, or fragment thereof that has specificity for an antigen…
The invention relates to G protein-coupled receptor (GPCR) microarrays on porous substrates for structural or functional analyses of GPCRs, and methods of preparing porous substrate surfaces for receiving membranes that comprise GPCRs. In one embodiment, a GPCR microarray of the…
Glass compositions that may be used to produce chemically strengthened glass sheets by ion exchange. The glass compositions are chosen to promote simultaneously high compressive stress and deep depth of layer or, alternatively, to reduce the time needed to ion exchange the glass…