Glasses comprising SiO 2 , Al 2 O 3 , and P 2 O 5 that are capable of chemical strengthened by ion exchange and having high damage resistance. These phosphate-containing glasses have a structure in which silica (SiO 2 ) is replaced by aluminum phosphate (AlPO 4 ) and/or boron…
Potuzak Marcel
Glass compositions that may be used to produce chemically strengthened glass sheets by ion exchange. The glass compositions are chosen to promote simultaneously high compressive stress and deep depth of layer or, alternatively, to reduce the time needed to ion exchange the glass…
A glass article including at least about 40 mol % SiO 2 and, optionally, a colorant imparting a preselected color is disclosed. In general, the glass includes, in mol %, from about 40-70 SiO 2 , 0-25 Al 2 O 3 , 0-10 B 2 O 3 ; 5-35 Na 2 O, 0-2.5 K 2 O, 0-8.5 MgO, 0-2 ZnO, 0-10% P…
Glasses comprising SiO 2 , Al 2 O 3 , and P 2 O 5 that are capable of chemical strengthened by ion exchange and having high damage resistance. These phosphate-containing glasses have a structure in which silica (SiO 2 ) is replaced by aluminum phosphate (AlPO 4 ) and/or boron…
Glasses comprising SiO 2 , AI 2 ,O 3 , and P 2 O 5 that are capable of chemical strengthened by ion exchange and having high damage resistance. These phosphate- containing glasses have a structure in which silica (SiO 2 ,) is replaced by aluminum phosphate (AIPO 4 ) and/or boron…
Described herein are alkali-free, boroalumino silicate glasses exhibiting desirable physical and chemical properties for use as substrates in flat panel display devices, such as, active matrix liquid crystal displays (AMLCDs) and active matrix organic light emitting diode…
Glass compositions that may be used to produce chemically strengthened glass sheets by ion exchange. The glass compositions are chosen to promote simultaneously high compressive stress and deep depth of layer or, alternatively, to reduce the time needed to ion exchange the glass…
A nano-porous composition, a substrate thereof, and an article thereof, that can be used, for example, for Surface Enhanced Raman spectroscopy (SERS), and like applications. The disclosure also provides methods of making the nano-porous compositions, articles, and methods for…
A method of making glass through a glass ribbon forming process in which a glass ribbon is drawn from a root point to an exit point is provided. The method comprises the steps of: (I) cooling the glass ribbon at a first cooling rate from an initial temperature to a process start…
Glass compositions that may be used to produce chemically strengthened glass sheets by ion exchange. The glass compositions are chosen to promote simultaneously high compressive stress and deep depth of layer or, alternatively, to reduce the time needed to ion exchange the glass…
A glass article including at least about 40 mol% SiO 2 and, optionally, a colorant imparting a preselected color is disclosed. In general, the glass includes, in mol%, from about 40-70 SiO 2 , 0-25 AI 2 O 3 , 0-10 B 2 O 3 ; 5-35 Na 2 O, 0-2.5 K 2 O, 0-8.5 MgO, 0-2 ZnO, 0-10% P 2…
A method of making glass through a glass ribbon forming process in which a glass ribbon is drawn from a root point to an exit point is provided. The method comprises the steps of: (I) cooling the glass ribbon at a first cooling rate from an initial temperature to a process start…
Ion exchangeable glasses that comprise at least one of a transition metal oxide or a rare earth oxide and have compositions that simultaneously promote a surface layer having a high compressive stress and deep depth of layer or, alternatively, reduced ion exchange time.
Computer-implemented methods and apparatus are provided for predicting/estimating (i) a non-equilibrium viscosity for at least one given time point in a given temperature profile for a given glass composition, (ii) at least one temperature profile that will provide a given…
Provided herein are substrates useful for surface-enhanced Raman spectroscopy (SERS), as well as methods of making substrates. The substrates comprise a support element; a nanoparticulate layer; a SERS-active layer in contact with said nanoparticulate layer; and optionally, an…
A glass article including at least about 40 mol% SiO 2 and, optionally, a colorant imparting a preselected color is disclosed. In general, the glass includes, in mol%, from about 40-70 SiO 2 , 0-25 AI 2 O 3 , 0-10 B 2 O 3 ; 5-35 Na 2 O, 0-2.5 K 2 O, 0-8.5 MgO, 0-2 ZnO, 0-10% P 2…
Ion exchangeable glasses that comprise at least one of a transition metal oxide or a rare earth oxide and have compositions that simultaneously promote a surface layer having a high compressive stress and deep depth of layer or, alternatively, reduced ion exchange time.