US 2007074841 A1#32523610 Most Cited · 3 citations0.2/yr · PR 1.09PendingUS · Application
Component forming method
Inventors: Voice Wayne E, Wu Xinhua, Loretto MichaelAssignee: Voice Wayne E, Wu XinhuaFiled 2006-10-02

A component can be formed by a hot isostatic pressing (HIP) process but it is necessary to reinforce intricate internal structures against collapse and deformation by the hot isostatic pressing process. The present method utilises a low melting point salt or alloy reinforcement…

US 2007175551 A1#102784283 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Method of heat treating titanium aluminide
Inventors: Voice Wayne E, Hu Dawei, Wu Xinhua, Loretto MichaelAssignee: Voice Wayne E, Hu DaweiFiled 2007-01-18

A gamma titanium aluminide alloy consisting of 46 at % aluminium, 8 at % tantalum and the balance titanium plus incidental impurities has an alpha transus temperature T α between 1310° C. and 1320° C. The gamma titanium aluminide alloy was heated to a temperature T 1 =1330° C.…

US 2008041506 A1#73036751 Most Cited · 0 citations0.0/yr · PR 0.56PendingUS · Application
Alloy and method of treating titanium aluminide

A method of treating a titanium aluminide alloy having a single alpha phase field and being capable of producing a massively transformed gamma microstructure by subjecting the alloy to a temperature cycle that produces the massively transformed microstructure having a refined…