The invention relates to a method for producing ethylene homopolymers and copolymers in a tubular reactor having at least two polymerisation zones, at temperatures of between 150° C. and 350° C. and pressures of between 500 and 5000 bar, using oxygen as an initiator. Said method…
Lars Wittkowski
Ethylene homopolymers and copolymers are prepared in a tube reactor at from 160° C. to 350° C. and pressures in the range from 500 to 5000 bar, with or without use of molar mass regulators, using a peroxide mixture comprising from 1 to 95 mol %, based on the total amount of the…
Cosmetic preparations comprising polyethylene waxes having improved organoleptic properties Cosmetic preparations and toothpastes, comprising polyethylene waxes, in particular micronized polyethylene waxes with improved organoleptic properties prepared by (co)polymerization of…
Emulsifiable ethylene polymers comprising copolymers of from 90 to 95% by weight of ethylene, from 4 to 10% by weight of one or more C 3 -C 12 alkenecarboxylic acids, and from 0 to 1.2% by weight of one or more tertiary esters of the corresponding C 3 -C 12 alkenecarboxylic…
Compounds which contain one or more groups of the formula (I) —CH 2 —CH(NR 1 R 2 )— (I) where R 1 and R 2 , independently of one another, are each hydrogen, C 1-20 -alkyl, C 6-18 -aryl, C 7-20 -alkaryl, C 7-20 -aralkyl or a polyamine radical, are prepared by reductive amination…
A process for preparing thixotropic agents comprising from 0.1 to 30% by weight of at least one ethylene terpolymer wax, from 5 to 70% by weight of at least one first solvent incompatible with the ethylene terpolymer wax, and from 5 to 85% by weight of at least one solvent…