Provided is a tempered glass having a compression stress layer in a surface thereof, comprising, as a glass composition in terms of mol %, 50 to 75% of SiO 2 , 3 to 13% of Al 2 O 3 , 0 to 1.5% of B 2 O 3 , 0 to 4% of Li 2 O, 7 to 20% of Na 2 O, 0.5 to 10% of K 2 O, 0.5 to 13% of…
Kawamoto Kosuke
Provided is a tempered glass having a compression stress layer in a surface thereof, comprising, as a glass composition in terms of mol %, 50 to 75% of SiO 2 , 3 to 13% of Al 2 O 3 , 0 to 1.5% of B 2 O 3 , 0 to 4% of Li 2 O, 7 to 20% of Na 2 O, 0 to 10% of K 2 O, 0.5 to 13% of…
This tempered glass has a compressive stress layer on the surface and is characterized by containing, as the glass composition and in mol %, 50 to 75% of SiO 2 , 3 to 13% of Al 2 O 3 , 0 to 1.5% of B 2 O 3 , 0 to 4% of Li 2 O, 7 to 20% of Na 2 O, 0.5 to 10% of K 2 O, 0.5 to 13%…
Provided is a Li 2 O—Al 2 O 3 —SiO 2 -based crystallized glass, comprising, as a composition in terms of mass %, 55 to 75% of SiO 2 , 20.5 to 27% of Al 2 O 3 , 2% or more of Li 2 O, 1.5 to 3% of TiO 2 , 3.8 to 5% of TiO 2 +ZrO 2 , and 0.1 to 0.5% of SnO 2 , and satisfying the…
Provided is a tempered glass sheet having a compression stress layer in a surface thereof, comprising, as a glass composition expressed in mass % in terms of oxides, 50 to 70% of SiO 2 , 5 to 20% of Al 2 O 3 , 0 to 5% of B 2 O 3 , 8 to 18% of Na 2 O, 2 to 9% of K 2 O, and 30 to…
An object of the present invention is to provide a Li 2 O—Al 2 O 3 —SiO 2 based crystallized glass with excellent bubble quality even without using As 2 O 3 or Sb 2 O 3 as a fining agent and a method for producing the same. The Li 2 O—Al 2 O 3 —SiO 2 based crystallized glass of…
Provided is a Li 2 O—Al 2 O 3 —SiO 2 -based crystallizable glass characterized by comprising, as a glass composition in terms of mass %, 55 to 75% of SiO 2 , 19 to 24% of Al 2 O 3 , 3 to 4% of Li 2 O, 1.5 to 2.8% of TiO 2 , 3.8 to 4.8% of TiO 2 +ZrO 2 , and 0.1 to 0.5% of SnO 2…
Provided is a Li 2 O—Al 2 O 3 —SiO 2 -based crystallized glass, comprising, as a composition in terms of mass %, 55 to 75% of SiO 2 , 20.5 to 27% of Al 2 O 3 , 2% or more of Li 2 O, 1.5 to 3% of TiO 2 , 3.8 to 5% of TiO 2 +ZrO 2 , and 0.1 to 0.5% of SnO 2 , and satisfying the…
A tempered glass has a compression stress layer in a surface thereof, and includes as a glass composition in terms of mol %, 50 to 75% of SiO 2 , 3 to 13% of Al 2 O 3 , 0 to 1.5% of B 2 O 3 , 0 to 4% of Li 2 O, 7 to 20 % of Na 2 O, 0 to 10 % of K 2 O, 0.5 to 13% of MgO, 0 to 6%…
This tempered glass plate has a compressive stress layer on the surface and is characterized by having a glass composition that contains, in mass% in terms of oxides, 50-70% of SiO 2 , 5-20% of Al 2 O 3 , 0-5% of B 2 O 3 , 8-18% of Na 2 O, 2-9% of K 2 O and 30-1,500 ppm of Fe 2…
Disclosed is Li 2 O-Al 2 O 3 -SiO 2 crystalline glass which is characterized by having a glass composition that contains, in mass%, 55-75% of SiO 2 , 19-24% of Al 2 O 3 , 3-4% of Li 2 O, 1.5-2.8% of TiO 2 , 3.8-4.8% of TiO 2 + ZrO 2 and 0.1-0.5% of SnO 2 , while satisfying the…
An object of the present invention is to provide a Li 2 O—Al 2 O 3 —SiO 2 based crystallized glass with excellent bubble quality even without using As 2 O 3 or Sb 2 O 3 as a fining agent and a method for producing the same. The Li 2 O—Al 2 O 3 —SiO 2 based crystallized glass of…
A Li 2 O-Al 2 O 3 -SiO 2 -based crystallized glass which has a compositional constitution comprising, in mass%, 55-75% of SiO 2 , 20.5-27% of Al 2 O 3 , 2% or more of Li 2 O, 1.5-3% of TiO 2 , TiO 2 and ZrO 2 in the total amount of 3.8-5% and 0.1-0.5% of SnO 2 and is…
Disclosed are a Li 2 O-Al 2 O 3 -SiO 2 based crystallised glass and a production method for the same, said glass having excellent foam quality without using As 2 O 3 or Sb 2 O 3 as a clarifying agent. The disclosed Li 2 O-Al 2 O 3 -SiO 2 contains virtually no As 2 O 3 or Sb 2 O…