Tempered glass and tempered glass sheet
Abstract
A tempered glass has a compression stress layer in a surface thereof, and includes as a glass composition in terms of mol %, 50 to 75% of SiO 2 , 3 to 13% of Al 2 O 3 , 0 to 1.5% of B 2 O 3 , 0 to 4% of Li 2 O, 7 to 20 % of Na 2 O, 0 to 10 % of K 2 O, 0.5 to 13% of MgO, 0 to 6% of CaO, and 0 to 4.5% of SrO. The tempered glass is substantially free of As 2 O 3 , Sb 2 O 3 , PbO, and F. The tempered glass has a molar ratio MgO/(MgO+Al 2 O 3 ) of 0.05 to 0.30.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 6.
Claims (2 — 1 Independent, 1 Dependent)
- Claim 1Independent Claim
A glass sheet to be tempered by being subjected to a tempering treatment, comprising, as a glass composition in terms of mol %, 50 to 75% of SiO 2 , 3 to 13% of Al 2 O 3 , 0 to 1.5% of B 2 O 3 , 0 to 4% of Li 2 O, 7 to 20% of Na 2 O, 0 to 10% of K 2 O, 0.5 to 13% of MgO, 0 to 6% of CaO, and 0 to 4.5% of SrO, wherein the glass sheet is substantially free of As 2 O 3 , Sb 2 O 3 , PbO, and F, and wherein the glass sheet has: a length of 500 mm or more, a width of 500 mm or more, a thickness of 1.5 mm or less, and an Fmax value of 5 MPa or less, wherein the Fmax value is a maximum value of residua
- Claim 2Depends on #1
The glass sheet to be tempered according to claim 1 , wherein the glass sheet comprises, as a glass composition
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (11)
Non-Patent Literature (2)
- International Search Report issued Apr. 10, 2012 in International (PCT) Application No. PCT/JP2012/050559.
- Tetsuro Izumitani et al., "New Glass and Physical Properties Thereof", First Edition, Management System Laboratory, Co., Ltd., Aug. 20, 1984, pp. 451-498 with partial translation.