In the manufacture of cast iron or steel shot containing less than 3 per cent carbon, cast iron is melted in a cupola furnace and after it has been run off, and whilst still fluid, it is alloyed with liquid steel and subsequently sprayed into water or the like. Silicon,…
Assignee / Organization
Josef Jacobs
23Total Forward Citations
7Indexed Patents
3Avg Citations / Patent
1Portfolio H-Index
Key Inventors: Jacobs Josef Josef Jacobs
In a process for the manufacture of cast iron or steel shot molten cast iron, to which may be added alloying metals such as 0-1 per cent Mn, 0-1,8 per cent Si, 0-0,5 per cent Ni, 0-0,4 per cent Cr and/or 0-0,3 per cent V, is incompletely blown until the carbon content is reduced…
10,110. Jacobs, J. April 29, 1911, [Convention date]. Void. [Published under Section 91 of the Act.] Rolling.-Cylinders of copper or copper alloys are polished by rotating them in contact with smooth rollers pressed heavily against them. A pressure of 40 kg. per square mm. is…