Improvements in or relating to the manufacture of cast iron or steel shot

22Forward Citations (#3782921 Global)
0.3/yrCitation Velocity (#25109616 Global)
1.79Citation PageRank (#17398420 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

In the manufacture of cast iron or steel shot containing less than 3 per cent carbon, cast iron is melted in a cupola furnace and after it has been run off, and whilst still fluid, it is alloyed with liquid steel and subsequently sprayed into water or the like. Silicon, manganese, nickel, chromium, vanadium or other quality-improving alloy substance may be added in liquid or solid form either to the liquid steel before alloying or to the liquid steel-iron alloy. Broken or unbroken shot may be kept at a temperature of 700-800 DEG C. for 1 hour and then chilled.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 22.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 22 total)

References Cited — Backward Prior Art (0)

No backward patent references recorded.