Patents
Assignee / Organization

Jokisch Torsten

239Total Forward Citations
43Indexed Patents
6Avg Citations / Patent
8Portfolio H-Index
US 2012267347 A1#1600936 Most Cited · 37 citations2.6/yr · PR 5.46PendingUS · Application
Method for welding workpieces made of highly heat-resistant superalloys, including a particular mass feed rate of the welding filler material

A welding method for welding workpieces made of highly heat-resistant superalloys is provided. The method includes generating a heat input zone on the workpiece surface by means of a heat source, feeding welding filler material into the heat input zone by means of a feeding…

US 2012179285 A1#2057012 Most Cited · 32 citations2.3/yr · PR 4.21PendingUS · Application
Automated repair method and system

A method and system for automated repair of a machine component is provided. According to the proposed method, a first geometry of the component, including a damaged portion of the component, is digitalized. A trough is then machined over the damaged portion of the component.…

US 2011089150 A1#3956793 Most Cited · 21 citations1.4/yr · PR 3.28PendingUS · Application
Method and Apparatus for Welding Workpieces of High-Temperature Superalloys

A welding apparatus for welding workpieces of high-temperature superalloys is provided. The welding apparatus includes a heat source for producing a heat input zone on the workpiece surface, a supplying device for supplying welding filler into the heat input zone and a…

WO 2011/054864 A1#4329941 Most Cited · 20 citations1.3/yr · PR 2.30PendingWO · Application
Single crystal welding of directionally solidified materials

The invention relates to the targeted selection of process parameters for laser welding, feeding, laser power beam diameter, and powder mass flow, wherein the temperature gradient substantially decisive for single crystal growth during laser application welding can be set…

US 2012273468 A1#5479940 Most Cited · 17 citations1.2/yr · PR 1.89PendingUS · Application
Single crystal welding of directionally solidified materials

A process for the directional solidification of a weld seam during build up welding is provided which includes the targeted selection of process parameters for laser welding, feeding, laser power beam diameter, and powder mass flow. The temperature gradient substantially…

US 2011073636 A1#7012212 Most Cited · 14 citations0.9/yr · PR 2.27PendingUS · Application
Method and device for welding workpieces made of high-temperature resistant super Alloys

A method of welding workpieces of high-temperature superalloys is provided. Welding filler is applied in a plurality of layers to a surface of the workpiece via a heat input zone and a supply zone for supplying the welding filler into the heat input zone. The heat input zone and…

US 2013268107 A1#8619911 Most Cited · 12 citations0.9/yr · PR 1.88PendingUS · Application
Surface analysis for detecting closed holes and method for reopening

By means of laser triangulation measurements of an uncoated and a coated component having holes, the exact positions of the holes can be detected for reopening after coating. A method for the surface analysis of at least partially closed holes which are to be opened is provided.…

WO 2010/112553 A2#9120785 Most Cited · 11 citations0.7/yr · PR 2.59PendingWO · Application
Welding method and component

During the filling of recesses (16) by welding, binding defects and cracks may appear. A suitable filling strategy in which welding material is also produced outside the recess (16), on the surface, enables said problems to be avoided.

US 2012103950 A1#13950913 Most Cited · 8 citations0.6/yr · PR 1.43PendingUS · Application
Welding method and component

A process for welding a component in which a recess is filled by welding tracks is provided. The process includes providing a recess with a contour which delimits an outer upper surface of the component with respect to the recess. The welding tracks are laid such that the…

US 8,437,010 B2#15690336 Most Cited · 7 citations0.5/yr · PR 1.58ActiveUS · Utility
Surface analysis for detecting closed holes, and device

A process for determining the position of closed holes in a component is provided. By carrying out laser triangulation measurements on an uncoated component and a coated component with holes, the exact position of the holes to be reopened may be detected following the coating. A…

WO 2009/143909 A1#15447217 Most Cited · 7 citations0.4/yr · PR 1.68PendingWO · Application
Method and device for welding workpieces made of high-temperature resistant super alloys

The present invention provides a welding device for welding workpieces (9) made of high-temperature resistant super alloys. The device comprises: - a heat source (3) for creating a heat application zone (11) on the workpiece surface (10); - a feed mechanism (5) for feeding…

US 2012268747 A1#18932368 Most Cited · 6 citations0.4/yr · PR 1.15PendingUS · Application
Surface analysis for detecting closed holes, and device

A process for determining the position of closed holes in a component is provided. By carrying out laser triangulation measurements on an uncoated component and a coated component with holes, the exact position of the holes to be reopened may be detected following the coating. A…

US 2014191017 A1#18405848 Most Cited · 6 citations0.5/yr · PR 1.43PendingUS · Application
Nickel-based alloy, use and method

The invention relates to a novel alloy which comprises the elements carbon (C), chromium (Cr), cobalt (Co), molybdenum (Mo), tungsten (W), titanium (Ti), aluminium (Al), boron (B), and zirconium (Zr), based on nickel, and which has a very low tendency to form cracks during…

US 8,996,156 B2#22471889 Most Cited · 5 citations0.5/yr · PR 1.09ActiveUS · Utility
Automated repair method and system

A method and system for automated repair of a machine component is provided. According to the proposed method, a first geometry of the component, including a damaged portion of the component, is digitalized. A trough is then machined over the damaged portion of the component.…

WO 2011/045343 A1#22355163 Most Cited · 5 citations0.3/yr · PR 1.16PendingWO · Application
Reference determination for ascertaining the positions of closed holes, device and machining device

By introducing fixed, yet removable pins (4, 4'') in a component (1, 120, 130, 155), the positions of drilling axes of holes (13, 13'') can be exactly ascertained by means of comparative measurement before and after the coating.

US 8,426,765 B2#27347641 Most Cited · 4 citations0.3/yr · PR 1.03ActiveUS · Utility
Method and apparatus for welding workpieces of high-temperature superalloys

A welding apparatus for welding workpieces of high-temperature superalloys is provided. The welding apparatus includes a heat source for producing a heat input zone on the workpiece surface, a supplying device for supplying welding filler into the heat input zone and a…

US 9,035,213 B2#27092068 Most Cited · 4 citations0.4/yr · PR 1.11ActiveUS · Utility
Method for welding workpieces made of highly heat-resistant superalloys, including a particular mass feed rate of the welding filler material

A welding method for welding workpieces made of highly heat-resistant superalloys is provided. The method includes generating a heat input zone on the workpiece surface by means of a heat source, feeding welding filler material into the heat input zone by means of a feeding…

US 2012211478 A1#31564850 Most Cited · 3 citations0.2/yr · PR 1.15PendingUS · Application
Multiple laser machining at different angles

A process using a single millisecond laser is presented. The process is traversed over the surface of a component a number of times. The tilt angle of the laser beam with respect to a drilling axis during a subsequent traverse is different from the tilt angle with respect to the…

US 2012263866 A1#28602984 Most Cited · 3 citations0.2/yr · PR 1.47PendingUS · Application
Method for measuring layer thickness by means of laser triangulation, and device

A method for determining the layer thickness of a component to be coated is provided. The monitoring of the process is automated by carrying out laser triangulation measurement before and after the coating of the component. At least one reference point on the component is used…

US 2012285933 A1#32988283 Most Cited · 3 citations0.2/yr · PR 1.07PendingUS · Application
Monocrystalline welding of directionally compacted materials

A method for directionally compacting a weld seam during build-up welding is provided. The method is used for the build-up welding of a component substrate that is compacted in a directional manner and comprises dendrites which extend in a substrate dendrite direction. The…

US 2013180108 A1#33643358 Most Cited · 3 citations0.2/yr · PR 1.02PendingUS · Application
Method for treating turbine blades and device therefor

A method is provided for treating turbine blades having holes for discharging cooling air. A protective layer is provided and then the holes that are partly or completely closed by the protective layer are opened again. Coordinates concerning the position of the holes are…

US 9,403,245 B2#33993226 Most Cited · 3 citations0.3/yr · PR 0.97ActiveUS · Utility
Method for treating turbine blades and device therefor
Inventors: Arjakine Nikolai, Melzer-jokisch Torsten, Thomaidis DimitriosAssignee: Arjakine Nikolai, Melzer-jokisch TorstenFiled 2011-09-14 · Granted 2016-08-02

A method is provided for treating turbine blades having holes for discharging cooling air. A protective layer is provided and then the holes that are partly or completely closed by the protective layer are opened again. Coordinates concerning the position of the holes are…

WO 2012/035060 A1#33741208 Most Cited · 3 citations0.2/yr · PR 1.01PendingWO · Application
Method for treating turbine blades and device therefor

The invention relates to a method for treating turbine blades (1) which have cooling air holes (2) for the discharge of cooling air, wherein a protective coating is applied and then the cooling air holes that are partially or completely closed by the protective coating are…

WO 2012/136471 A1#30942395 Most Cited · 3 citations0.2/yr · PR 1.18PendingWO · Application
Method for determining a coating thickness

The invention relates to a method for determining the thickness of the coating applied to a component during a component coating process, comprising the following steps: defining a coordinate origin, in particular at a position of the component to be coated that is not subject…

US 2014123890 A1#42094620 Most Cited · 2 citations0.2/yr · PR 0.96PendingUS · Application
Single-crystal welding of directionally compacted materials

A process for welding directionally solidified metallic materials is presented. Process parameters are targeted selected with respect to laser welding, advancement, laser power beam diameter and powder mass flow. The temperature gradient, which is fundamentally decisive for the…