By means of laser triangulation measurements of an uncoated and a coated component having holes, the exact positions of the holes can be detected for reopening after coating. A method for the surface analysis of at least partially closed holes which are to be opened is provided.…
Oppert Andreas
Method for repairing turbine blades that have a film cooling opening (418) or cylindrical opening and are intended with a coating, comprises completely removing the coating from the turbine blades and applying a new ceramic or metallic laminar coating (2, 3) on the turbine…
A process for determining the position of closed holes in a component is provided. By carrying out laser triangulation measurements on an uncoated component and a coated component with holes, the exact position of the holes to be reopened may be detected following the coating. A…
The method involves measuring a component with opened holes (7', 7'') in an uncoated condition, and producing a masking model by a laser triangulation measurement, where the masking model contains positions of the holes and orientation of longitudinal axes of the…
A process for determining the position of closed holes in a component is provided. By carrying out laser triangulation measurements on an uncoated component and a coated component with holes, the exact position of the holes to be reopened may be detected following the coating. A…
A method for reprocessing a turbine blade having at least one platform which due to the action of corrosion is undersized on at least one lateral platform face is provided. According to the method, the target dimension of the platform is restored by applying material to the at…
A method for the production of a hole (19) in a component (1) by means of a focused beam (13) which has a specific cross-sectional surface (A), particularly a specific diameter (d) on the plane of the surface (22) of the component (1), wherein the cross-sectional surface (A),…
The method involves measuring a component (1) e.g. turbine blades (120, 130) and heat shielding element (155), before and during or after coating by laser triangulation. Layer thickness of the component is calculated from different measurements. Laser triangulation measurement…
By introducing fixed, yet removable pins (4, 4'') in a component (1, 120, 130, 155), the positions of drilling axes of holes (13, 13'') can be exactly ascertained by means of comparative measurement before and after the coating.
The invention relates to a method for reprocessing a turbine blade having at least one platform (7) which due to the action of corrosion is undersized on at least one lateral platform face (9, 11). According to the method, the target dimension of the platform (7) is restored by…
The method involves measuring a rotor blade (120) and a stator blade (130) of a gas turbine with unclosed holes in an uncoated condition. A mask model (19) is generated by laser triangulation, where the mask model contains position of the holes and orientation of longitudinal…
The method involves measuring a component with the non-closed holes in the uncoated state and generating a mask model (19). The mask model is generated by measuring through laser triangulation. The laser triangulation includes the position of the holes and the orientation of…
Production of a hole (19) in a component (1) using a focused beam (13) comprises directing the beam within the component or within a wall to be penetrated in a first process step. Preferred Features: The focus of the beam is shifted during the production of the hole from the…
The method for reference layer determination of cooling vents (13', 13") partially connected on components (1, 120, 130, 155) to be coated, comprises detachably and tightly mounting two cylindrical-shaped pins (4', 4") on the component, measuring the layers of…
A process for making a hole into a substrate by a laser is provided. According to the proposed process, in a first step, at least one intermediate hole is produced into the substrate by at least one laser, the intermediate hole having an intermediate diameter that is smaller…
A process using a single millisecond laser is presented. The process is traversed over the surface of a component a number of times. The tilt angle of the laser beam with respect to a drilling axis during a subsequent traverse is different from the tilt angle with respect to the…
A method for determining the layer thickness of a component to be coated is provided. The monitoring of the process is automated by carrying out laser triangulation measurement before and after the coating of the component. At least one reference point on the component is used…
A process for making a hole into a substrate by at least one laser includes a first step which involves producing at least one intermediate hole with a diameter which is smaller than a final diameter of a final hole to be produced. The intermediate hole with the smaller diameter…
Deepish cracks (4) can not be repaired with conventional techniques such as for example laser plasma welding since the crack (4) is not completely fused to the depth of the crack and thus sealed. According to the invention the method using filler materials (7) increase the…
The invention relates to a method for determining the thickness of the coating applied to a component during a component coating process, comprising the following steps: defining a coordinate origin, in particular at a position of the component to be coated that is not subject…
The present invention relates to laser drilling without burr formation. In a percussion process for producing a hole, burrs are often formed. The formation of burrs is prevented by a percussion process in a first step and a trepanning process in a second step, wherein the…
The method involves producing the normal size of the platform (7) in the undersize, and carrying out a material (12) application on a platform side surface (9,11) in the undersize, such that an oversize of the platform exists after the material application and finally the…
The method of producing hole (10) by a laser, comprises producing an intermediate hole (10') with significantly smaller diameter in comparison with a hole to be produced, and producing a final diameter of the hole to be produced. The intermediate hole represents a blind hole…
The device has a holder or support for a component i.e. turbine blade, to be processed (4). A water jet nozzle is provided with a variable water jet (7) that flow in and flow out such that a sensor is able to receive acoustic signals of a contact point of water jet with the…
By carrying out laser triangulation measurements on an uncoated component and a coated component with holes, the exact position of the holes to be reopened can be detected following the coating.