Patents
Assignee / Organization

Gehrmann Bodo

34Total Forward Citations
15Indexed Patents
2Avg Citations / Patent
3Portfolio H-Index
WO 2009/135469 A1#10402694 Most Cited · 10 citations0.6/yr · PR 2.14PendingWO · Application
Iron-nickel alloy
Inventors: De Boer Bernd, Gehrmann BodoAssignee: Thyssenkrupp Vdm Gmbh, De Boer BerndFiled 2009-04-29

The invention relates to an iron-nickel alloy with the following composition (in % by mass): C 0.05 to 0.5 % Cr 0.2 to 2.0 % Ni 33 to 42 % Mn < 0.1 % Si < 0.1 % Mo 1.5 to 4.0 % Nb 0.01 to 0.5 % AI 0.1 to 0.8 % Mg 0.001 to 0.01 % V max. 0.1 % W 0.1 to 1.5 % Co max. 2.0 % Fe…

US 2009047167 A1#15094297 Most Cited · 7 citations0.4/yr · PR 1.84PendingUS · Application
Iron-Nickel Alloy
Inventors: Gehrmann Bodo, Boer BerndAssignee: Gehrmann Bodo, Boer BerndFiled 2007-01-26

Disclosed is a creep-resistant low-expansion iron-nickel alloy that is provided with increased mechanical resistance and contains 40 to 43 wt. % of Ni, a maximum of 0.1 wt. % of C, 2.0 to 3.5 wt. % of Ti, 0.1 to 1.5 wt. % of Al, 0.1 to 1.0 wt. % of Nb, 0.005 to 0.8 wt. % of Mn,…

WO 2007/087785 A1#19919309 Most Cited · 5 citations0.3/yr · PR 1.75PendingWO · Application
Iron-nickel alloy
Inventors: Gehrmann Bodo, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Gehrmann BodoFiled 2007-01-26

Disclosed is a creep-resistant low-expansion iron-nickel alloy that is provided with increased mechanical resistance and contains 40 to 43 wt. % of Ni, a maximum of 0.1 wt. % of C, 2.0 to 3.5 wt. % of Ti, 0.1 to 1.5 wt. % of Al, 0.1 to 1.0 wt. % of Nb, 0.005 to 0.8 wt. % of Mn,…

WO 2007/087786 A1#28370913 Most Cited · 3 citations0.2/yr · PR 1.54PendingWO · Application
Iron-nickel-cobalt alloy
Inventors: Gehrmann Bodo, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Gehrmann BodoFiled 2007-01-26

Use of an iron-nickel-cobalt alloy in CFC mould construction comprising (in % by mass) Ni from 30 to 35%, Co from 3 to 6%, Al from 0.001 to 0.1%, Mn from 0.005 to 0.5%, Si from 0.005 to 0.5%, C max. 0.1%, balance Fe and constituents resulting from production, with the alloy…

US 2010175847 A1#40236461 Most Cited · 2 citations0.1/yr · PR 1.00PendingUS · Application
Iron-Nickel-Cobalt Alloy
Inventors: Gehrmann Bodo, Boer BerndAssignee: Gehrmann Bodo, Boer BerndFiled 2007-01-26

Use of an iron-nickel-cobalt alloy in CFC mould construction comprising (in % by mass) Ni from 30 to 35%, Co from 3 to 6%, Al from 0.001 to 0.1%, Mn from 0.005 to 0.5%, Si from 0.005 to 0.5%, C max. 0.1%, balance Fe and constituents resulting from production, with the alloy…

US 8,808,475 B2#43625965 Most Cited · 2 citations0.2/yr · PR 0.93ActiveUS · Utility
Iron-nickel alloy
Inventors: Gehrmann Bodo, Boer BerndAssignee: Gehrmann Bodo, Boer BerndFiled 2007-01-26 · Granted 2014-08-19

Disclosed is a creep-resistant low-expansion iron-nickel alloy that is provided with increased mechanical resistance and contains 40 to 43 wt. % of Ni, a maximum of 0.1 wt. % of C, 2.0 to 3.5 wt. % of Ti, 0.1 to 1.5 wt. % of Al, 0.1 to 1.0 wt. % of Nb, 0.005 to 0.8 wt. % of Mn,…

WO 0,107,673 A1#40111209 Most Cited · 2 citations0.1/yr · PR 1.01PendingWO · Application
Iron-nickel alloy with creep resistance and low thermal expansion

The invention relates to iron-nickel alloys with creep resistance and low thermal expansion, which contain ( % by mass) no more than about 0.2 % C, no more than 0.3 % Mn, no more than 0,3 % Si, from 0.05 to 3.0 % Al, 0.1 to 3.0 % Ti, no more than 1.0 % Nb, from 39.0 to 45.0 %…

WO 0,121,848 A1#59023509 Most Cited · 1 citations0.0/yr · PR 0.78PendingWO · Application
Iron-nickel alloy with low thermal expansion coefficient and exceptional mechanical properties
Inventors: Gehrmann Bodo, Erpenbeck BurkhardAssignee: Krupp Vdm Gmbh, Gehrmann BodoFiled 2000-08-03

The invention relates to creep-resistant iron-nickel alloys with a low expansion coefficient that contain (in weight %), in addition to 0.02 to 0.3 % C, a maximum of 1 % Mn, and a maximum of 1 % Si, an Mo content of 0.1 to 2.5 % and/or a Cr content of 0.1 to 2.5 % ≤1.0 % Nb, as…

WO 2004/053179 A1#48293234 Most Cited · 1 citations0.1/yr · PR 0.92PendingWO · Application
Iron-nickel-cobalt alloy, method for the production and use thereof

The invention relates to an iron-nickel-cobalt alloy for masking shadow which is used for large-sized monitors and flat screens. The inventive alloy has the following chemical composition: 32,5-34.5 mass % Ni, 3.0-4.5 mass % Co, maximum of 0.1mass % Mo, maximum of 0.1mass % Cr,…

WO 2008/125091 A2#59240758 Most Cited · 1 citations0.1/yr · PR 0.78PendingWO · Application
Metal foil

The invention relates to a metal foil having (in weight %) Ni 74 - 90%, W 10 - 26%, and Al and/or Mg and/or B contents of Al > 0 - max. 0.02%, Mg > 0 - max. 0.025%, B > 0 - max. 0.005%.

WO 0,066,802 A1#88617706 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Iron-nickel alloy
Inventors: Gehrmann BodoAssignee: Krupp Vdm Gmbh, Gehrmann BodoFiled 2000-02-02

The invention relates to a low-expansion iron-nickel alloy, which to adjust a coefficient of thermal expansion of < 0.6 x 10-6/K at between 20 and 100 °C contains (in % by mass) in addition to up to 0.009 % C, up to 0.1 % Mn, up to 0.1 % Si and up to 0.1 % Al, between 0.5 and…

WO 03,025,232 A1#76726474 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method for producing a metal strip from an iron-nickel alloy for tensioned shadow masks

The invention relates to a method for producing a strip from an iron-nickel alloy for tensioned shadow masks used in flat monitors and display screens, whereby the strip comprised of a chemical composition (in mass %) 35-38 % Ni, 0.4-0.8 % Mo, 0.1-0.3 % Cr, 0.08-0.12 % C, max. 1…

WO 2007/087786 A8#68177382 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Iron-nickel-cobalt alloy
Inventors: Gehrmann Bodo, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Gehrmann BodoFiled 2007-01-26

Use of an iron-nickel-cobalt alloy in CFC mould construction comprising (in % by mass) Ni from 30 to 35%, Co from 3 to 6%, Al from 0.001 to 0.1%, Mn from 0.005 to 0.5%, Si from 0.005 to 0.5%, C max. 0.1%, balance Fe and constituents resulting from production, with the alloy…

WO 2008/125091 A3#132102734 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Metal foil

The invention relates to a metal foil having (in weight %) Ni 74 - 90%, W 10 - 26%, and Al and/or Mg and/or B contents of Al > 0 - max. 0.02%, Mg > 0 - max. 0.025%, B > 0 - max. 0.005%.

WO 9,737,361 A1#147379690 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Low-retentivity nickel-ion alloy

The invention relates to a low-retentivity nickel-iron-molybdenum alloy with an inital magnetic permeability ν4 > 280,000 and maximum magnetic permeability νmax > 400,000 obtainable by deoxidising the melt metal with aluminium and/or silicon and limiting the magnesium…