WO 2009/135469 A1#10402694 Most Cited · 10 citations0.6/yr · PR 2.14PendingWO · Application
Iron-nickel alloy
Inventors: De Boer Bernd, Gehrmann BodoAssignee: Thyssenkrupp Vdm Gmbh, De Boer BerndFiled 2009-04-29

The invention relates to an iron-nickel alloy with the following composition (in % by mass): C 0.05 to 0.5 % Cr 0.2 to 2.0 % Ni 33 to 42 % Mn < 0.1 % Si < 0.1 % Mo 1.5 to 4.0 % Nb 0.01 to 0.5 % AI 0.1 to 0.8 % Mg 0.001 to 0.01 % V max. 0.1 % W 0.1 to 1.5 % Co max. 2.0 % Fe…

US 2009047167 A1#15094297 Most Cited · 7 citations0.4/yr · PR 1.84PendingUS · Application
Iron-Nickel Alloy
Inventors: Gehrmann Bodo, Boer BerndAssignee: Gehrmann Bodo, Boer BerndFiled 2007-01-26

Disclosed is a creep-resistant low-expansion iron-nickel alloy that is provided with increased mechanical resistance and contains 40 to 43 wt. % of Ni, a maximum of 0.1 wt. % of C, 2.0 to 3.5 wt. % of Ti, 0.1 to 1.5 wt. % of Al, 0.1 to 1.0 wt. % of Nb, 0.005 to 0.8 wt. % of Mn,…

WO 2007/087785 A1#19919309 Most Cited · 5 citations0.3/yr · PR 1.75PendingWO · Application
Iron-nickel alloy
Inventors: Gehrmann Bodo, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Gehrmann BodoFiled 2007-01-26

Disclosed is a creep-resistant low-expansion iron-nickel alloy that is provided with increased mechanical resistance and contains 40 to 43 wt. % of Ni, a maximum of 0.1 wt. % of C, 2.0 to 3.5 wt. % of Ti, 0.1 to 1.5 wt. % of Al, 0.1 to 1.0 wt. % of Nb, 0.005 to 0.8 wt. % of Mn,…

US 2010310412 A1#26418605 Most Cited · 4 citations0.2/yr · PR 1.20PendingUS · Application
Austenitic heat-resistant nickel-base alloy

Austentic heat-resistant nickel-base alloy comprising (in % by mass) 0.03-0.1% of C, 28-32% of Cr, 0.01-<0.5% of Mn, 0.01-<0.3% of Si, 0.01-<1.0% of Mo, 2.5-3.2% of Ti, 0.01-<0.5% of Nb, 0.01-<0.5% of Cu, 0.05-<2.0% of Fe, 0.7-1.0% of Al, 0.001-<0.03% of Mg,…

WO 2007/087786 A1#28370913 Most Cited · 3 citations0.2/yr · PR 1.54PendingWO · Application
Iron-nickel-cobalt alloy
Inventors: Gehrmann Bodo, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Gehrmann BodoFiled 2007-01-26

Use of an iron-nickel-cobalt alloy in CFC mould construction comprising (in % by mass) Ni from 30 to 35%, Co from 3 to 6%, Al from 0.001 to 0.1%, Mn from 0.005 to 0.5%, Si from 0.005 to 0.5%, C max. 0.1%, balance Fe and constituents resulting from production, with the alloy…

US 2010175847 A1#40236461 Most Cited · 2 citations0.1/yr · PR 1.00PendingUS · Application
Iron-Nickel-Cobalt Alloy
Inventors: Gehrmann Bodo, Boer BerndAssignee: Gehrmann Bodo, Boer BerndFiled 2007-01-26

Use of an iron-nickel-cobalt alloy in CFC mould construction comprising (in % by mass) Ni from 30 to 35%, Co from 3 to 6%, Al from 0.001 to 0.1%, Mn from 0.005 to 0.5%, Si from 0.005 to 0.5%, C max. 0.1%, balance Fe and constituents resulting from production, with the alloy…

US 8,808,475 B2#43625965 Most Cited · 2 citations0.2/yr · PR 0.93ActiveUS · Utility
Iron-nickel alloy
Inventors: Gehrmann Bodo, Boer BerndAssignee: Gehrmann Bodo, Boer BerndFiled 2007-01-26 · Granted 2014-08-19

Disclosed is a creep-resistant low-expansion iron-nickel alloy that is provided with increased mechanical resistance and contains 40 to 43 wt. % of Ni, a maximum of 0.1 wt. % of C, 2.0 to 3.5 wt. % of Ti, 0.1 to 1.5 wt. % of Al, 0.1 to 1.0 wt. % of Nb, 0.005 to 0.8 wt. % of Mn,…

US 8,889,066 B2#40892814 Most Cited · 2 citations0.2/yr · PR 0.99ActiveUS · Utility
Iron-nickel alloy with a high level of ductility and a low expansion coefficient
Inventors: Hoberg Bernd, De Boer BerndAssignee: Hoberg Bernd, De Boer BerndFiled 2007-10-20 · Granted 2014-11-18

The invention relates to a solid-solution strengthened iron-nickel alloy with a high level of ductility and an expansion coefficient <5×10 −6 /K in the temperature range between room temperature and −200° C. Said alloy consists of (in wt. %): between 0.005 and 0.05% of C;…

WO 0,246,108 A2#67858627 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Metal strip for epitaxial coatings and method for the production thereof

The aim of the invention is to provide a metal strip for epitaxial coating with a biaxially textured layer, this metal strip, however, being able to be produced in an uncomplicated manner and having a high tensile strength, low magnetic losses and/or a high electrical…

WO 0,246,108 A3#126663087 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredWO · Utility
Metal strip for epitaxial coatings and method for the production thereof

The aim of the invention is to provide a metal strip for epitaxial coating with a biaxially textured layer, this metal strip, however, being able to be produced in an uncomplicated manner and having a high tensile strength, low magnetic losses and/or a high electrical…

WO 03,060,203 A1#126368225 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Metal strip for epitaxial coating and method for production thereof

The invention relates to a metal strip made from a layer composite for epitaxial coating and a method for production thereof. The aim of the invention is to produce such a high-strength metal strip and a corresponding production method. Said metal strip is a layer composite made…

WO 2007/087786 A8#68177382 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Iron-nickel-cobalt alloy
Inventors: Gehrmann Bodo, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Gehrmann BodoFiled 2007-01-26

Use of an iron-nickel-cobalt alloy in CFC mould construction comprising (in % by mass) Ni from 30 to 35%, Co from 3 to 6%, Al from 0.001 to 0.1%, Mn from 0.005 to 0.5%, Si from 0.005 to 0.5%, C max. 0.1%, balance Fe and constituents resulting from production, with the alloy…

WO 2008/064624 A2#147909458 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Iron-nickel alloy with a high level of ductility and a low expansion coefficient
Inventors: Hoberg Bernd, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Hoberg BerndFiled 2007-10-20

The invention relates to a solid-solution strengthened iron-nickel alloy with a high level of ductility and an expansion coefficient < 5 X 10<SUP>-6</SUP>/K in the temperature range between room temperature and - 200 °C. Said alloy consists of (in wt. %): between…

WO 2008/064624 A3#137608831 Most Cited · 0 citations0.0/yr · PR 0.56ActiveWO · Utility
Iron-nickel alloy with a high level of ductility and a low expansion coefficient
Inventors: Hoberg Bernd, De Boer BerndAssignee: Thyssenkrupp Vdm Gmbh, Hoberg BerndFiled 2007-10-20

The invention relates to a solid-solution strengthened iron-nickel alloy with a high level of ductility and an expansion coefficient < 5 x 10-6/K in the temperature range between room temperature and - 200 °C. Said alloy consists of (in wt. %): between 0.005 and 0.05 % of C;…

WO 2009/079972 A1#102926865 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Austenitic heat-resistant nickel-base alloy

Austenitic heat-resistant nickel-base alloy comprising (in % by mass) 0.03-0.1% of C, 28-32% of Cr, 0.01-≤ 0.5% of Mn, 0.01-≤ 0.3% of Si, 0.01-≤ 1.0% of Mo, 2.5-3.2% of Ti, 0.01-≤ 0.5% of Nb, 0.01-≤ 0.5% of Cu, 0.05-≤ 2.0% of Fe, 0.7-1.0% of Al, 0.001-≤ 0.03% of Mg, 0.01-≤ 1.0%…