An article of manufacture selected from a titanium alloy fastener and a titanium alloy fastener stock including an alpha/beta titanium alloy comprising, in percent by weight: 3.9 to 5.4 aluminum; 2.2 to 3.0 vanadium; 1.2 to 1.8 iron; 0.24 to 0.3 oxygen; up to 0.08 carbon; up to…
Bryan David J
An article of manufacture selected from a titanium alloy fastener and a titanium alloy fastener stock including an alpha/beta titanium alloy comprising, in percent by weight: 3.9 to 4.5 aluminum; 2.2 to 3.0 vanadium; 1.2 to 1.8 iron; 0.24 to 0.3 oxygen; up to 0.08 carbon; up to…
Processes for forming an article from an α+β titanium alloy are disclosed. The α+β titanium alloy includes, in weight percentages, from 2.90 to 5.00 aluminum, from 2.00 to 3.00 vanadium, from 0.40 to 2.00 iron, and from 0.10 to 0.30 oxygen. The α+β titanium alloy is cold worked…
Processes for forming an article from an α+β titanium alloy are disclosed. The α+β titanium alloy includes, in weight percentages, from 2.90 to 5.00 aluminum, from 2.00 to 3.00 vanadium, from 0.40 to 2.00 iron, and from 0.10 to 0.30 oxygen. The α+β titanium alloy is cold worked…
A method for straightening a solution treated and aged (STA) titanium alloy form includes heating an STA titanium alloy form to a straightening temperature of at least 25° F. below the age hardening temperature, and applying an elongation tensile stress for a time sufficient to…
Oxidation resistant niobium based alloys have a composition to provide a stable ternary phase such as PtYAl or PdYAl, which supplies yttrium and aluminum to the system and forms a protective oxide such as Yttria-Aluminum-Garnet (YAG) scale at elevated temperature. These niobium…
An alpha/beta titanium alloy comprising, in percent by weight based on total alloy weight: 3.9 to 4.5 aluminum; 2.2 to 3.0 vanadium; 1.2 to 1.8 iron; 0.24 to 0.30 oxygen; up to 0.08 carbon; up to 0.05 nitrogen; up to 0.015 hydrogen ; titanium; and up to a total of 0.30 of other…
An alpha/beta titanium alloy comprising, in percent by weight based on total alloy weight: 3.9 to 4.5 aluminum; 2.2 to 3.0 vanadium; 1.2 to 1.8 iron; 0.24 to 0.30 oxygen; up to 0.08 carbon; up to 0.05 nitrogen; up to 0.015 hydrogen; titanium; and up to a total of 0.30 of other…
Processes for forming an article from an α+β titanium alloy are disclosed. The α+β titanium alloy includes, in weight percentages, from 2.90 to 5.00 aluminum, from 2.00 to 3.00 vanadium, from 0.40 to 2.00 iron, and from 0.10 to 0.30 oxygen. The α+β titanium alloy is cold worked…
An article of manufacture selected from a titanium alloy fastener and a titanium alloy fastener stock including an alpha/beta titanium alloy comprising, in percent by weight: 3.9 to 4.5 aluminum; 2.2 to 3.0 vanadium; 1.2 to 1.8 iron; 0.24 to 0.3 oxygen; up to 0.08 carbon; up to…
Certain embodiments of a method for increasing the strength and toughness of a titanium alloy include plastically deforming a titanium alloy at a temperature in an alpha-beta phase field of the titanium alloy to an equivalent plastic deformation of at least a 25% reduction in…
An article of manufacture selected from a titanium alloy fastener and a titanium alloy fastener stock including an alpha/beta titanium alloy comprising, in percent by weight: 3.9 to 4.5 aluminum; 2.2 to 3.0 vanadium; 1.2 to 1.8 iron; 0.24 to 0.3 oxygen; up to 0.08 carbon; up to…
A method for straightening a solution treated and aged (STA) titanium alloy form includes heating an STA titanium alloy form to a straightening temperature of at least 25° F. below the age hardening temperature, and applying an elongation tensile stress for a time sufficient to…
Certain embodiments of a method for increasing the strength and toughness of a titanium alloy include plastically deforming a titanium alloy at a temperature in an alpha-beta phase field of the titanium alloy to an equivalent plastic deformation of at least a 25% reduction in…
Certain embodiments of a method for increasing the strength and toughness of a titanium alloy include plastically deforming a titanium alloy at a temperature in an alpha-beta phase field of the titanium alloy to an equivalent plastic deformation of at least a 25% reduction in…
A method for straightening a solution treated and aged (STA) titanium alloy form includes heating an STA titanium alloy form to a straightening temperature of at least 25°F below the age hardening temperature, and applying an elongation tensile stress for a time sufficient to…