A method for increasing the tensile strength of a cold-workable α - β titanium alloy is disclosed, comprising β -106 ℃ to T β -solution heat treating a cold-workable α - β titanium alloy at a temperature in the range of 72.2 ℃ for 15 minutes to 2 hours, cooling the α - β…
Ati Properties Llc
Processes for forming an article from an α+β titanium alloy are disclosed. The α+β titanium alloy includes, in weight percentages, from 2.90 to 5.00 aluminum, from 2.00 to 3.00 vanadium, from 0.40 to 2.00 iron, and from 0.10 to 0.30 oxygen. The α+β titanium alloy is cold worked…
A method for heat treating a powder metallurgy nickel-base alloy article includes placing the article in a furnace at an initial temperature in the furnace that is 80 ℃ to 200 ℃ below a gamma prime solvus temperature, and increasing the temperature in the furnace to a solvus…
One embodiment of a method of refining alpha-phase grain size in an alpha-beta titanium alloy comprises working an alpha-beta titanium alloy at a first working temperature within a first temperature range in the alpha-beta phase field of the alpha-beta titanium alloy. The alloy…
A non-limiting embodiment of a titanium alloy comprises, in weight percentages based on total alloy weight: 2.0 to 5.0 aluminum; 3.0 to 8.0 tin; 1.0 to 5.0 zirconium; 0 to a total of 16.0 of one or more elements selected from the group consisting of oxygen, vanadium, molybdenum,…
A method of producing a seamless, composite tubular product includes centrifugally casting a metal or alloy into a tubular workpiece having an inner diameter. The method then centrifugally casts a corrosion resistant alloy in the inner diameter of the tubular workpiece to form a…
A method of melting and refining an alloy comprises vacuum induction melting starting materials to provide a vacuum induction melted alloy. At least a portion of the vacuum induction melted alloy is electroslag remelted to provide an electroslag remelted alloy. At least a…
An austenitic stainless steel comprises, by weight, 9 to 23% chromium, 30 to 35% nickel, 1 to 6% molybdenum, 0 to 0.03% titanium, 0.15% to 0.6% aluminum, up to 0.1% carbon, 1 to 1.5% manganese, 0 to less than 0.8% silicon, 0.25 to 0.6% niobium and iron. Embodiments of austenitic…
Nickel-based alloys having improved localized corrosion resistance, improved stress-corrosion cracking (SCC) resistance and impact strength are disclosed. The improvements come from the provision of compositions that are resistant to deleterious phase formation and from the…
Processes for the production of tantalum alloys and niobium are disclosed. The processes use aluminothermic reactions to reduce tantalum pentoxide to tantalum metal or niobium pentoxide to niobium metal.
An alpha-beta titanium alloy comprises, in weight percentages: an aluminum equivalency in the range of 2.0 to 10.0; a molybdenum equivalency in the range of 0 to 20.0; 0.3 to 5.0 cobalt; and titanium. In certain embodiments, the alpha-beta titanium alloy exhibits a cold working…
A method for making a tube is described in which a multi-layer billet is extruded to provide a tube having a wall comprising an inner layer metallurgically bonded to an outer layer.
A method of producing a beta-titanium alloy elongated product form having a chemical composition as specified in UNS R58150 or ASTM F2066-13. The method comprises solution treating, aging, straightening, stress-relief aging, and cooling the elongated product form. Articles of…
The present invention relates to a non-limiting embodiment of a titanium alloy comprising, in weight percent based on total alloy weight: 2.0 to 5.0 aluminum; 3.0 to 8.0 tin; 1.0 to 5.0 zirconium; 0 to a total of 16.0 of one or more elements selected from the group consisting of…
A method of melting and refining an alloy comprises vacuum induction melting starting materials to provide a vacuum induction melted alloy. At least a portion of the vacuum induction melted alloy is electroslag remelted to provide an electroslag remelted alloy. At least a…
PROBLEM TO BE SOLVED: To provide an improved design for corrosion resistant fluid conducting parts for equipment that operates under conditions promoting corrosion during urea synthesis, and to provide a method for retrofitting worn and/or corrosion-prone parts of existing…
PROBLEM TO BE SOLVED: To provide a more effective and/or more cost-effective method of hot-working crack sensitive alloys.SOLUTION: A method of processing an alloy ingot or other alloy workpiece to reduce thermal cracking comprises disposing a glass fiber fabric on the alloy…
To provide a process for producing titanium alloys having coarse, fine, very fine, or ultrafine grain microstructure that does not require multiple reheats, accommodates higher strain rates, reduces the time necessary for processing, and eliminates the need for custom forging…
합금을 용해 및 정련하는 방법은 출발 물질을 진공 유도 용해시켜 진공 유도 용해된 합금을 제공하는 단계를 포함한다. 진공 유도 용해된 합금의 적어도 일부분은 일렉트로슬래그 재용해되어 일렉트로슬래그 재용해된 합금을 제공한다. 진공 아크 재용해된 합금의 적어도 일부분은 진공 아크 재용해되어 단일 진공 아크 재용해된 합금을 제공한다. 단일 진공 아크 재용해된 합금의 적어도 일부분은 진공 아크 재용해되어 이중 진공 아크 재용해된 합금을 제공한다. 다양한 실시형태에서, 진공 유도 용해된 합금의 조성은…
A method of producing an article selected from a titanium article and a titanium alloy article comprises melting feed materials with a source of hydrogen to form a molten heat of titanium or a titanium alloy, and casting at least a portion of the molten heat to form a…
A method of producing a bimetallic tubular component includes providing a first tubular workpiece having an inner diameter and a second tubular workpiece having an outer diameter. The first and second tubular workpieces have dissimilar cold-working processing parameters. The…