The present invention relates to a cutting insert for turning in steel, stainless steel and heat resistant super alloys comprising a substrate and a coating. The insert has a rake face (1), a flank face (2), cutting edges (3) and a cutting corner (4). The cemented carbide…
Aakesson Leif
The present invention relates to a coated cemented carbide insert with a binder phase enriched surface zone. The WC-grains have an average grain size in the range 1.0-3.5 νm, preferably 1.3-3.0 νm and the number of WC-grains larger than 2 times the average grain size is less…
Borehole opener, particularly for enlarging this hole underneath a casing in the field of oil prospecting, comprising a body ( 2 ) of longitudinal axis ( 3 ), a duct ( 4 ) for drilling fluid, formed longitudinally in the body ( 2 ), and at least two hole-opening arms ( 5 ) which…
The present invention relates to coated cutting tool inserts particularly useful for heavy roughing turning operations of very large steel components, such as drive shafts for ships and shafts for wind power plants. The inserts are large with an iC, inscribed circle diameter, of…
The present invention relates to a method of sintering cemented carbide bodies including heating said bodies to the sintering temperature in a suitable atmosphere and cooling. If said cooling at least to below 1200 °C is performed in a hydrogen atmosphere of pressure 0.4-0.9 bar…
The invention relates to a borehole underreamer, in particular for a hole below a well casing in the field of oil exploration, comprising a longitudinal body, a drilling fluid conduit, which is disposed longitudinally in the body and which is provided with a fluid flow section…
The present invention relates to a WC-Co cemented carbide alloy. By adding an extremely small amount of Ti, V, Zr, Ta or Nb or a combination of these, a grain refined cemented carbide structure with less abnormal WC-grains has been obtained.
The present invention relates to a method of sintering cemented carbide bodies including heating said bodies to the sintering temperature in a suitable atmosphere and cooling. If said cooling at least to below 1200 °C is performed in a hydrogen atmosphere of pressure 0.4-0.9 bar…