The present invention relates to a cemented carbide insert with excellent properties for machining of steels and stainless steels. The cemented carbide comprises WC and 4-25 wt.% Co. The WC-grains have an average grain size in the range 0.2-3.5 νm and a narrow grain size…
Waldenstroem Mats
The present invention relates to a method of making bodies by powder metallurgical methods consiting of wet milling in an alcohol-water solution of a powder mixture containing hard constituents with sizes up to 2 νm, preferably up to 1 νm and binder phase, drying the milled…
The present invention relates to a cemented carbide body comprising WC with an average grain size of < 10 νm in a binder phase. In the cemented carbide body the WC grains can be classified in at least two groups in which a group of smaller grains has a maximum grain size amax…
The present invention relates to a method of making a powder mixture containing hard constituents based on carbides, nitrides and/or carbonitrides of Ti, Zr, Hf, V, Nb, Ta, Cr, Mo and/or W in a binder phase essentially based on Co and/or Ni and further containing particles up to…
The present invention relates to a method of making a cemented carbide by mixing powder of WC and possibly other powders forming hard constituents and binder phase and pressing agent, drying, pressing and sintering whereby; the mixing is wet mixing with no change in grain size…
The present invention relates to a coated cemented carbide insert with a binder phase enriched surface zone. The WC-grains have an average grain size in the range 1.0-3.5 νm, preferably 1.3-3.0 νm and the number of WC-grains larger than 2 times the average grain size is less…