THE MELTING TEMPERATURE OF THE RESIN; THE MOLDING PRESSURE OF ABOUT 3000 P.S.I. IS APPLIED TO THE MOLD BEFORE THE RESIN HAS TIME TO ENCAPSULATE THE FILLER; AFTER COOLING THE MOLD WHILE MAINTAINING THE PRESSURE, THE MOLDED STRUCTURE IS REMOVED FROM THE MOLD. A NOVEL MOLDED…
15 patent(s) · 3.1 ms · Refine in Advanced Search →
This disclosure describes a graphite composition and a fabrication procedure for producing coolant and/or support plates for acid fuel cells. The composition consists of a graphite powder sized principally in the 50 to 150 micron range with about seven percent of the graphite…
A thin electrochemical cell separator plate with greatly improved properties is made by molding and then graphitizing a mixture of preferably 50 percent high purity graphite powder and 50 percent carbonizable thermosetting phenolic resin, the graphite molding powder particles…